Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (11): 1-8    DOI:
Current Issue | Archive | Adv Search |
ANALYSIS ON VALENCE ELECTRON STRUCTURE OF Fe_3Al INTERMETALLIC COMPOUNDS
YIN Yansheng;SUN Yangshan;XIONG Hongqi;SHI Zhongliang;ZHANG Lining;SU Huaqin Dalian University of Technology Southeastern University; Nanjing
Cite this article: 

YIN Yansheng;SUN Yangshan;XIONG Hongqi;SHI Zhongliang;ZHANG Lining;SU Huaqin Dalian University of Technology Southeastern University; Nanjing. ANALYSIS ON VALENCE ELECTRON STRUCTURE OF Fe_3Al INTERMETALLIC COMPOUNDS. Acta Metall Sin, 1993, 29(11): 1-8.

Download:  PDF(590KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the empirical electron theory of solids and molecules, the analysison valence electron structure is made to Fe_3Al intermetallic compounds. The bonding com-plex model of DO_3 cell is set up. Some preliminary attempts at revealing the relationship be-tween alloy composition-structure-property and Fe_3Al alloy phase valence electron structureare presented.
Key words:  Fe_3Al      valence electron      bond structure     
Received:  18 November 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I11/1

1 余瑞璜.科学通报,1978;23(4) :271
2 余瑞璜.金属学报,1982;18(3) :A336
3 Lamy H J, Kayser F X. Phys Status solidi, 1969; 34: 765
4 Ehles S K, Mendiratta M, G. Air Force Wright Aeronautical laboratories, 1982; TR-82-4089
5 刘志林.合金价电子结构与成分设计.长春:吉林科技出版社,1990:3
6 余瑞璜.科学通报,1978;23:217
7 孙扬善.金属学报,1991;27(4) :A25
[1] Rui YANG,Yan PAN,Wei CHEN,Qiaoyan SUN,Lin XIAO,Jun SUN. DEFORMATION BEHAVIOR AND THE MECHANISM OF MICRO-SCALE Ti-10V-2Fe-3Al PILLARSIN COMPRESSION[J]. 金属学报, 2016, 52(2): 135-142.
[2] HUANG Lian, GAO Kunyuan, WEN Shengping, HUANG Hui, WANG Wei, NIE Zuoren. VALENCE ELECTRON STRUCTURE ANALYSIS OF EQUILIBRIUM AND METASTABLE PHASES OF Al3M(M=Ti, Zr, Hf)[J]. 金属学报, 2012, 48(4): 492-501.
[3] PENG Ke; YI Maozhong; RAN Liping. Analysis of Valence Electronic Structures and Properties of MoSi2 And WSi2[J]. 金属学报, 2006, 42(11): 1125-1129 .
[4] LIU Zhilin; LIU Weidong; LIN Cheng. STRENGTH CALCULATION AND ITS PREDICTION OF NON QUENCHED-TEMPERED STEEL DURING CONTINUOUS CASTING-ROLLING[J]. 金属学报, 2004, 40(12): 1248-1252 .
[5] YU Xinquan;SUN Yangshan;MEI Jianping;SUN Guoxiong (Department of Materials Science and Engineering;Southeast University; Nanjing 210096). ELECTRICAL PROPERTIES OF Fe_3Al INTERMETALLICS[J]. 金属学报, 1998, 34(11): 1126-1130.
[6] ZHENG Weiwei;YANG Wangyue;LIU Qing;SUN Zuqing(Department of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083). ROOM TEMPERATURE MECHANICAL BEHAVIOR OF B2-ORDERED Fe_3Al SINGLE CRYSTALS[J]. 金属学报, 1998, 34(11): 1137-1142.
[7] SUN Yangshan;YU Xinquan;HUANG Haibo;SUN Guoxiong (Department of Materials Science and Engineering; Southeast University; Nanjing 210096). OXIDATION RESISTANCE OF Fe_3Al INTERMETALLICS AT HIGH TEMPERATURES[J]. 金属学报, 1998, 34(11): 1131-1136.
[8] ZHANG Zhonghua; SUN Yangshan; LIU Guijun (Southeast University; Nanjing 210096). IMPROVEMENT OF ROOM TEMPERATURE ENVIRONMENTAL BRITTLEMENT OF Fe_3Al-BASED ALLOY BY ELECTRO-BRUSH PLATING[J]. 金属学报, 1996, 32(9): 955-958.
[9] YANG Wangyue; SHENG Lizhen;SUN Zuqing; HUANG Yuanding; MAO Weimin (University of Science and Technology Beijing; Beijing 100083); ZHANG Baisheng; YE Chuntang (China Institute of Atomic Energy; Beijing 102413)(Manuscript received 1995-11-10; in revised form 1996-04-05). NEUTRON DIFFRACTION STUDY ON SITE OCCUPATION OF SUBSTITUTIONAL ELEMENTS AT SUBLATTICE IN Fe_3Al INTERMETALLICS[J]. 金属学报, 1996, 32(8): 799-804.
[10] WENG Jun; ZHU Fengwu; ZHI Rentao; WANG Shuangquan; XIAO jimei (University of Scicnce and Technology Beijing; Beijing 100083)(Manuscript received 1995-12-18). FIM OBSERVATION ON B2 ORDERING IN Fe_3Al ALLOY[J]. 金属学报, 1996, 32(7): 695-699.
[11] ZHAO Zhongtao; LIU Tao; MA Ruzhang (University of Scicnce and Technology Beijing; Beijing 100083); MA Changying (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081 ). ON THE PRECIPITATE IN Fe-28Al ALLOY[J]. 金属学报, 1996, 32(6): 585-588.
[12] ZHU Ruifu; LU Yupeng; CHEN Chuanzhong; LI Shitong; WANG Shiqing (Shandong University of Technology; Jinan 250061) ZHANG Fucheng (Yanshan University; Qinhuangdao 066004). AN ANALYSIS OF VALENCE ELECTRON STRUCTURE OF Fe-C-Mn ALLOYING AUSTENITE[J]. 金属学报, 1996, 32(6): 561-564.
[13] CHEN Yanglin (Zhejiang University; Hangzhou 310027) (Manuscript received 1995-09-12; in revised form 1996-01-19). EFFECTS OF In ADDITION ON Pd HYDRIDING[J]. 金属学报, 1996, 32(5): 489-494.
[14] ZHANG Jianmin(Central Iron and Steel Research Institute;Ministry;of Metallurgical Industry;Beijing 100081)ZHANG Ruilin;YU Ruihuang(Jilin University;Changchun 130023)(Manuscript received 1994-08-29;in revised form 1995-02-05). HYDROGEN EMBRITTLEMENT BEHAVIOUR IN Fe_3Al[J]. 金属学报, 1995, 31(7): 300-303.
[15] LI Musen; FU Shaoli(Shandong University of Technology; Jinan 250014). XU Wandong(Tianjin University; Mianjin 300072); ZHANG Ruilin. YU Ruihuang(Jilin University; Changchun 130023). VALENCE ELECTRON STRUCTURE OF Fe_2B PHASE AND ITS EIGEN-BRITTLENESS[J]. 金属学报, 1995, 31(5): 201-208.
No Suggested Reading articles found!