| EQUILIBRIA OF SYSTEM MoO_3-MoO_2-H_2O-H_2 AND PHASE DIAGRAM FOR SYSTEM Mo-O BETWEEN 400 AND 700℃ |
| FANG Zheng;CHEN Xinmin Central South University of Technology; Changsha |
|
Cite this article:
FANG Zheng;CHEN Xinmin Central South University of Technology; Changsha. EQUILIBRIA OF SYSTEM MoO_3-MoO_2-H_2O-H_2 AND PHASE DIAGRAM FOR SYSTEM Mo-O BETWEEN 400 AND 700℃. Acta Metall Sin, 1993, 29(11): 54-59.
|
|
|
Abstract The equilibria of the system MoO_3-MoO_2-H_2O-H_2 were investigated usinga specially designed thermogravimetric apparatus under the control of atmospheres. The equi-librium constants for the reaction MoO_3+H_2=MoO_2+H_2O(g) were measured at P_(H_2O)/p_(H_2) ratio between 0.412 and 0.609 and in the temperature range of 400 to 534℃ as follows:lg(p_(H_2O)/ P_(H_2)=0.702-739.8/T.The standard enthalpy of formation and absoluteentropy forMoO_3 at 298.15 K have been evaluated as-854.75kJ/mole and 78.16 J/Kmole respectively. The experimental results show that the magneli phases in theMoO_3-MoO_2 system cannot exist as the thermodynamically stable phases under the condi-tions studied. The phase diagram of the system Mo-O between 400 and 700℃ has also beengiven.
|
|
Received: 18 November 1993
|
1 方正.博士学位论文,中南工业大学,1987. 6 2 方正,陈新民.金属学报,1989;25:B221 3 Kihlborg L. Acta Chem Scand, 1959; 13: 954 4 #12 5 Phillips B, Chang L L Y. Trans AIME, 1965; 233: 1434 6 Sardi A. Acta Chim Hung, 1963; 38: 177, 39: 145 7 Kubaschewshi O, Alcock C B. Metallurgical Thermochemistry, 5th ed, New York: Pergamon Press, 1979: 380 8 Jordannov CH V, Nikolov T G, Cimbulev M T. Neue Hutte, 1968; 13:215 9 方正,陈新民.中南矿冶学院学报,1982;13(4) :1 10 Barin I, Knacke O. Thermochemical Properties of Inorganic Sub-stances, New York: Pergamon Press, 1973 11 Rapp R A. Physicochemical Measurements in Metals Research, Vol. 4(1) , New York: Interscience, 1970 12 Staskiewicz B A, Tucker J R, Snyder P E. J Am Chem Soc, 1955; 77: 2987 13 Mah A D. J Phys Chem, 1957; 61: 1572 14 Kelley K K, King E G. Bur Mines Bull, 1961:592 15 方正,张平民,陈新民.金属学报,1990;26:B92 16 Phillips B, Chang L L Y, Phase Diagrams for Ceramists, 1975 Supplement, Ed by Levin E M, Mcmurdie H F, Natl Bur Stad, 1975:9R |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|