| INFLUENCE OF ELECTROMAGNETIC STIRRING ON MACRO-SEGREGATION OF GREY CAST IRON |
| CAO Zhiqiang;ZHANG Liping;REN Zhongming;JIN Junze Dalian University of Technology |
|
Cite this article:
CAO Zhiqiang;ZHANG Liping;REN Zhongming;JIN Junze Dalian University of Technology. INFLUENCE OF ELECTROMAGNETIC STIRRING ON MACRO-SEGREGATION OF GREY CAST IRON. Acta Metall Sin, 1992, 28(2): 82-85.
|
|
|
Abstract Enrichment of massive graphite on lateral surface and evident macro--segrega-tion along both longitudinal and axial directions were found by the influence of intense electromagnetic stirring during unidirectionally solidifying grey cast iron ingot. A secondaryflow within the region near solid--liquid interface seems to be the cause of axial segregation, and the solidification rate may also be influential to the macro--segregation.
|
|
Received: 18 February 1992
|
1 Shingu P H, Kurosaki M, Jin-Junze. Trans Jpn Inst Met, 1986; 27: 546 2 任忠鸣,苏辉,金俊泽.金属学报,1990;26:B 374 3 Wetterfall S-E, Fredriksson H, Hillert M. J Iron Steel Inst, 1972; 210: 323 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|