| INFLUENCE OF PHYSICAL DAMAGE EFFECT OF PSB ON CRACK INITIATION IN Al SINGLE CRYSTAL |
| ZHAI Tongguang;LIN Shi;PAN Hu;XIAO Jimei University of Science and Technology Beijing |
|
Cite this article:
ZHAI Tongguang;LIN Shi;PAN Hu;XIAO Jimei University of Science and Technology Beijing. INFLUENCE OF PHYSICAL DAMAGE EFFECT OF PSB ON CRACK INITIATION IN Al SINGLE CRYSTAL. Acta Metall Sin, 1991, 27(1): 32-38.
|
|
|
Abstract An investigation was made of the crack initiation by cyclic deforma-tion on the two special surfaces of pure Al single crystal. One is the tOp-surfaeccontaining the active Burger's vector, and the other is the top-surface formingthe smallest angle with the active Burger's vector. The fatigue test were performedat the constant resolved shear stress amplitude (5 Pa), zero mean stress. Expe-rimentel results show that many microcracks are initiated on the side-surface onwhich no PSB surface topographies are formed during cyclic deformation. Cracks onthe side-surface are short with mean length of about 10 μm and distributed appro-ximately in a similar direction, perpendicular to the active Burger's vector, whereason the top-surface cracks are not as obvious as those on the side-surface. Observa-tions by scanning acoustic microscopy show that the fatigue damage on the side-surface is much deeper than that on the top-surface. A model of crack nucleationby voiding, and of PSB formation is suggested.
|
|
Received: 18 January 1991
|
1 Mughrabi H, Wang R, Differt K et al. ASTM STP 811, 1983: 5 2 Mughrabi H. In: McQueen H J, Bailon J-P, Dickson J I et al. eds. Strength of Metals and Alloys (ICSMA7) , Vol. III, Proc 7th Int Conf on the Strength of Metals and Alloys, Montreal, Canada, 12--16 Augest, 1985, Oxford: Pergamon, 1986: 1917 3 Neumann P. In: Cahn R W. Haasen P eds. Fatigue, Physical Matallurgy, 3rd ed, New York: Elsevier Science, 1983: 1553 4 Brown L M. In: Ashby M F, Bullough R, Hartley C S et al. eds. Dislocation Modelling of Physical Systems, Proc Int Conf, Gainesville, Florida USA, 22--27 June, 1980, Oxford: Pergamon, 1981: 51 5 Essmann U, Goesele U, Mughrabi H. Philos Mag, 1981; A44: 405 6 Smith G C. Mater Sci Technol, 1986; 2: 881 7 Vorren O. Ryum N. Acta Metall, 1987; 35: 855 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|