MICROSTRUCTURE AND PHASE COMPOSITION OF SOLIDIFIED Ni-BASE SUPERALLOY POWDER
HU Benfu;LI Huiying;WU Chengjian;ZHANG Shouhua University of Science and Technology Beijing
Cite this article: 

HU Benfu;LI Huiying;WU Chengjian;ZHANG Shouhua University of Science and Technology Beijing. MICROSTRUCTURE AND PHASE COMPOSITION OF SOLIDIFIED Ni-BASE SUPERALLOY POWDER. Acta Metall Sin, 1990, 26(5): 22-27.

Download:  PDF(2087KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure and phase composition of FGH95 Ni-base super-alloy powder of different mesh size solidified from chemical deposition of prealloy-ed Ni have been investigated. The microstructure transition was found from dendrite inmajor into cellular precipitate as the reduction of powder size and the increase ofcooling rate. The principal phase was identified as different morphologies of MC-type carbides, which may be related to their composition and the condition of solid-ification. Minor phases, such as Laves, primary γ' and boride are also present,and they exist as associated with carbides.
Key words:  powder metallugy      superalloy      microstructure      solidification     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/22

1 Tien J K, Boesch W J, Howson T E, Castledine W B. P/M Superalloy Technology and Applications, 1980 International Powder Metallurgy Conference, 22--27 June 1980, Washington, preprint
2 胡本芙,李慧英,章守华.金属学报,1987;23:B95
3 Smugeresky J F. Metall Trans, 1982; 13A: 1535
4 黄乾尧.钢铁,1981;16:41
5 Fernandez R, Lecomte T C, Kattamis T Z. Metall Trans, 1978; 9A: 1381
6 李慧英,胡本芙,章守华.金属学报,1987;23:B91
7 Ingesten N G, Warren R, Winberg L. In: Brunetaud R, Coutsouradis D, Gibbons T B, Lindblom Y, Meadowcroft D B, Stickler R eds.. High Temperature Alloys for Gas Turbines, 1982, Proc of a Conf, Held in Liege, Belgium, 4--6 October, 1982, Dordrecht, Holl and: D Reidel, 1982: 1013
8 Dahlen M, Fischmeister H. In: Tien J K, Wlodek S T, Morrow H III, Gell M, Maurer G eds., Superalloys 1980, Proc 4th Int Symposium on Superalloys, 21--25 September 1980, Champion, Pennsylvania, Metals Park, Ohio: ASM, 1980: 44
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[4] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[6] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[7] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[8] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[9] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[10] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[11] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[12] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[13] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[14] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[15] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
No Suggested Reading articles found!