CONTACTING FATIGUE FAILURE OF Cu-22% Pb PLAIN BEARING ALLOY
JIA Jun;CHEN Xianchao Harbin Institute of Technology
Cite this article: 

JIA Jun;CHEN Xianchao Harbin Institute of Technology. CONTACTING FATIGUE FAILURE OF Cu-22% Pb PLAIN BEARING ALLOY. Acta Metall Sin, 1989, 25(3): 76-78.

Download:  PDF(1539KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The results of the contacting fatigue tests for Cu-22%Pb plain bearing alloyshow that the fatigue failure behavior of the alloy is related to the distribution of Pb particles.Both the additions of mischmetal and sulphure can refine the Pb paticles. However, mischmetalimproves and sulphur deteriorates the fatigue property of the alloy.
Key words:  Cu-Pb alloy      contacting fatigue      crack initiation      crack propagation     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/76

1 《铸造有色合金及其熔炼》联合编写组编.铸造有色合金及其熔炼,北京:国防工业出版社,1980:149
2 蔡泽高,刘以宽,王承忠,郑文龙,金属磨损与断裂,上海交通大学出版社,1985:231
3 Knight R J. Foundry, 1962; (10) : 46
4 Burgardt W, Schwietzke G. Giesserei, 1968; 55: 350
5 邱聿成.铸造,1983;(5) :27
[1] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[2] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[3] ZHOU Hongwei, BAI Fengmei, YANG Lei, CHEN Yan, FANG Junfei, ZHANG Liqiang, YI Hailong, HE Yizhu. Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel[J]. 金属学报, 2020, 56(7): 937-948.
[4] Bin CHEN,Jie HE,Xiaojun SUN,Jiuzhou ZHAO,Hongxiang JIANG,Lili ZHANG,Hongri HAO. Liquid-Liquid Phase Separation of Fe-Cu-Pb Alloy and Its Application in Metal Separation and Recycling of Waste Printed Circuit Boards[J]. 金属学报, 2019, 55(6): 751-761.
[5] ZHANG Xiaochen, MENG Weiying, ZOU Defang, ZHOU Peng, SHI Huaitao. Effect of Pre-Cyclic Stress on Fatigue Crack Propagation Behavior of Key Structural Al Alloy Materials Used in High Speed Trains[J]. 金属学报, 2019, 55(10): 1243-1250.
[6] Jin WANG, Liming YU, Yuan HUANG, Huijun LI, Yongchang LIU. Effect of Crystal Orientation and He Density on Crack Propagation Behavior of bcc-Fe[J]. 金属学报, 2018, 54(1): 47-54.
[7] Shu GUO,En-Hou HAN,Haitao WANG,Zhiming ZHANG,Jianqiu WANG. Life Prediction for Stress Corrosion Behavior of 316L Stainless Steel Elbow of Nuclear Power Plant[J]. 金属学报, 2017, 53(4): 455-464.
[8] Zhiyong LIU,Zongshu LI,Xiaolin ZHAN,Wenzhu HUANGFU,Cuiwei DU,Xiaogang LI. GROWTH BEHAVIOR AND MECHANISM OF STRESS CORROSION CRACKS OF X80 PIPELINE STEEL IN SIMULATED YINGTAN SOIL SOLUTION[J]. 金属学报, 2016, 52(8): 965-972.
[9] Li WANG,Zhongjiao ZHOU,Shaohua ZHANG,Xiangdong JIANG,Langhong LOU,Jian ZHANG. CRACK INITIATION AND PROPAGATION AROUND HOLES OF Ni-BASED SINGLE CRYSTAL SUPERALLOY DURING THERMAL FATIGUE CYCLE[J]. 金属学报, 2015, 51(10): 1273-1278.
[10] YU Long, SONG Xiping, ZHANG Min, LI Hongliang, JIAO Zehui, YU Huichen. CRACK INITIATION AND PROPAGATION OF HIGH Nb-CONTAINING TiAl ALLOY IN FATIGUE-CREEP INTERACTION[J]. 金属学报, 2014, 50(10): 1253-1259.
[11] WANG Zhiying WANG Jianqiu HAN En–hou KE Wei YAN Maocheng ZHANG Junwei LIU Chuwei . STRESS CORROSION CRACK INITIATION BEHAVIOR FOR THE X70 PIPELINE STEEL BENEATH A DISBONDED COATING[J]. 金属学报, 2012, 48(10): 1267-1272.
[12] JIANG Bing XING Xianran GUO Zhimeng. CRACK PROPAGATION AND DOMAIN SWITCHING IN BaTiO3 SINGLE CRYSTALS UNDER EXTERNAL FIELD[J]. 金属学报, 2011, 47(5): 605-610.
[13] ZHOU Yanlei XU Yang CHEN Jun LIU Zhenyu. EXPERIMENTAL STUDY OF THE IMPACT FRACTURE BEHAVIOR OF FH550 OFFSHORE PLATFORM STEEL[J]. 金属学报, 2011, 47(11): 1382-1387.
[14] XIE Jijia HONG Youshi. EXPERIMENTAL INVESTIGATION ON FATIGUE BEHAVIOR OF NANOCRYSTALLINE NICKEL[J]. 金属学报, 2009, 45(7): 844-848.
[15] ZHANG Yongjian HUI Weijun XIANG Jinzhong DONG Han WENG Yuqing . EFFECT OF GRAIN SIZE ON ULTRA--HIGH--CYCLE FATIGUE PROPERTIES OF 42CrMoVNb STEEL[J]. 金属学报, 2009, 45(7): 880-886.
No Suggested Reading articles found!