| CRACK PROPAGATION AND DOMAIN SWITCHING IN BaTiO3 SINGLE CRYSTALS UNDER EXTERNAL FIELD |
| JIANG Bing1), XING Xianran1), GUO Zhimeng2) |
1) School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083
2) Advanced Material and Technology Institute, University of Science and Technology Beijing, Beijing 100083 |
|
Cite this article:
JIANG Bing XING Xianran GUO Zhimeng. CRACK PROPAGATION AND DOMAIN SWITCHING IN BaTiO3 SINGLE CRYSTALS UNDER EXTERNAL FIELD. Acta Metall Sin, 2011, 47(5): 605-610.
|
|
|
Abstract Domain switching and crack propagation in BaTiO3 single crystal under external field were in-situ observed by polarized light microscopy (PLM). It was found that under mechanical field, domain-switching bands appear around the crack tip to relax stress and domain switching occurred before crack propagation. Under electric field, the internal stress induced by domain switching results in crack propagation.
|
|
Received: 09 December 2010
|
| Fund: Supported by National Natural Science Foundation of China (No.50571011) and China Postdoctoral Science Foundation (No.2010048019) |
| [1] Yang W. Mechatronic Reliability. Beijing: Tsinghua University Press, 2001: 1(杨卫. 力电失效学. 北京: 清华大学出版社, 2001: 1)[2] Lynch C S. Acta Mater, 1996, 44: 4137[3] Lu W, Fang D N, Hwang K C. Acta Mater, 1999; 47: 2913[4] Li F X, Rajapakse R K N D. Acta Mater, 2007; 55: 6472[5] Shaikh M G, Phanish S. Sivakumar S M. Comput Mater Sci, 2006; 37: 178[6] Tang L P, Xie S H, Zheng X J, Zhou Y C, Li J Y. Mech Mater, 2008; 40: 362[7] Tan X, Shang J K. J Appl Phys, 2004, 96: 2805[8] Zhang Z K, Fang D N, Soh A K. Mech Mater, 2006; 38: 25[9] Roelofs A, Bottger U, Waser R. Appl Phys Lett, 2000; 77: 3444[10] Shin S, Baek J, Hong J W, Khim Z G. J Appl Phys, 2004; 96: 4372[11] Jiang B, Bai Y, Chu W Y, Shi S Q, Qiao L J. Su Y J. Appl Phys Lett, 2008; 93: 152905[12] Zhang Z H, Qi X Y, Duan X F. Appl Phys Lett, 2006; 89: 242905[13] Park J H, Park J, Lee K B. Appl Phys Lett, 2007; 91: 012906[14] Fang F, Yang W, Zhang F C, Luo H S. J Am Ceram Soc, 2005; 88: 2491[15] Huang H Y, Chu W Y, Su Y J, Qiao L J, Gao K W. Mater Sci Eng, 2005; B122: 1[16] Wang F, Su Y J, He J Y, Qiao L J, Chu W Y. Scr Mater, 2006; 54: 201[17] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. Appl Phys Lett, 2003; 82: 1583[18] Kounga Njiwa A B, Lupascu D C, Rodel J. Acta Mater, 2004; 52: 4919[19] Hwang S C, Lynch C S, McMeeking R M. Acta Metall Mater, 1995; 43: 2073[20] Meschke F, Kollek A, Schneider G A. J Eur Ceram Soc, 1997; 17: 1143[21] Busche M J, Hsia K J. Scr Mater, 2001; 44: 207[22] Beom H G, Kang K J. Acta Mech, 2006; 185: 201[23] Jiang Y J, Fang D N, Li F X. Appl Phys Lett, 2007; 90: 222907[24] Jiang B, Bai Y, Cao J L, Su Y J, Shi S Q, Chu W Y, Qiao L J. J Appl Phys, 2008; 103: 116102[25] Jiang B, Bai Y, Chu W Y, Shi S Q, Qiao L J. Su Y J. Appl Surf Sci, 2008; 254: 5594[26] Huang K Z, Wang Z Q. Macro–Micro–Mechanics and Strengthening and Toughening Design of Materials, Beijing: Tsinghua University Press, 2003: 182(黄克智, 王自强. 材料的宏微观力学与强韧化设计. 北京: 清华大学出版社, 2003: 182)[27] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Sensitive Fracture. Beijing: Science Press, 2000: 77(褚武扬, 乔利杰, 陈奇志, 高克玮. 断裂与环境断裂. 北京: 科学出版社, 2000: 77) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|