IN SITU OBSERVATION OF CRACK TIP DEFORMATION IN A DUPLEX STAINLESS STEEL
YAO Kefu;TANG Naiyong;CHEN Nanping Tsinghua University
Cite this article: 

YAO Kefu;TANG Naiyong;CHEN Nanping Tsinghua University. IN SITU OBSERVATION OF CRACK TIP DEFORMATION IN A DUPLEX STAINLESS STEEL. Acta Metall Sin, 1989, 25(3): 57-62.

Download:  PDF(3243KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In the ferrite grains, the dislocation emitted by the crack tips maycross-slip out of the original slip planes and form a broad plastic zone. However, inaustenite, the dislocation free zone is small and the dislocations emittee by the crackpile-up in its slip plane. The selection of the slip planes at the crack tip depend onthe Schmid factor of crack tip in both phases. But after large deformation, the se-lection of the second slip systems at the crack tip in austenite does not depend on theSchmid factor.
Key words:  crack tip      dislocation configuration Schmid factor      duplex stainless steel     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/57

1 Rice J R, Rosengren G F. J Mech Phys Solids, 1968; 16: 1
2 Hutchinson J W. J Mech Phys Solids, 1968; 16: 13
3 Gardner R N, Wilsdoif H G F. Metall Trans, 1980; 11A: 653
4 Ohr S M. Mater Sci Eng, 1985; 72: 1
5 张以增,戴蜀娟,邹鸿承,苗丕峰,理化检验(物理分册),1985;22(5) :19
6 姚可夫,唐迺泳,陈南平.第五届全国断裂力学会议文集,桂林,1988:156
[1] CHEN Guo, WANG Xinbo, ZHANG Renxiao, MA Chengyue, YANG Haifeng, ZHOU Li, ZHAO Yunqiang. Effect of Tool Rotation Speed on Microstructure and Properties of Friction Stir Processed 2507 Duplex Stainless Steel[J]. 金属学报, 2021, 57(6): 725-735.
[2] NI Ke, YANG Yinhui, CAO Jianchun, WANG Liuhang, LIU Zehui, QIAN Hao. Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. 金属学报, 2021, 57(2): 224-236.
[3] DENG Yahui, YANG Yinhui, PU Chaobo, NI Ke, PAN Xiaoyu. Effect of Mn Addition on High Temperature Tensile Behavior of 23%Cr Low Nickel Type Duplex Stainless Steel[J]. 金属学报, 2020, 56(7): 949-959.
[4] WANG Guiqin,WANG Qin,CHE Honglong,LI Yajun,LEI Mingkai. Effects of Silicon on the Microstructure and Propertiesof Cast Duplex Stainless Steel with Ultra-HighChromium and High Carbon[J]. 金属学报, 2020, 56(3): 278-290.
[5] Miao JIN, Wenquan LI, Shuo HAO, Ruixue MEI, Na LI, Lei CHEN. Effect of Solution Temperature on Tensile Deformation Behavior of Mn-N Bearing Duplex Stainless Steel[J]. 金属学报, 2019, 55(4): 436-444.
[6] Yahui DENG,Yinhui YANG,Jianchun CAO,Hao QIAN. Research on Dynamic Recrystallization Behavior of 23Cr-2.2Ni-6.3Mn-0.26N Low Nickel TypeDuplex Stainless Steel[J]. 金属学报, 2019, 55(4): 445-456.
[7] CHEN Lei , HAO Shuo , MEI Ruixue , JIA Wei , LI Wenquan , GUO Baofeng . Intrinsic Increment of Plasticity Induced by TRIP and Its Dependence on the Annealing Temperature in a Lean Duplex Stainless Steel[J]. 金属学报, 2019, 55(11): 1359-1366.
[8] Yusen SU, Yinhui YANG, Jianchun CAO, Yuliang BAI. Research on Hot Working Behavior of Low-NickelDuplex Stainless Steel 2101[J]. 金属学报, 2018, 54(4): 485-493.
[9] Hai ZHANG,Shilei LI,Gang LIU,Yanli WANG. Effects of Hot Working on the Microstructure and Thermal Ageing Impact Fracture Behaviors of Z3CN20-09MDuplex Stainless Steel[J]. 金属学报, 2017, 53(5): 531-538.
[10] Yulai CHEN,Zhaoyin LUO,Jingyuan LI. EFFECT OF SOLUTION TEMPERATURE ON MICRO- STRUCTURE AND PITTING CORROSION RESISTANCE OF S32760 DUPLEX STAINLESS STEEL[J]. 金属学报, 2015, 51(9): 1085-1091.
[11] DAI Fuzhi, ZHANG Wenzheng. AN INVESTIGATION ON THE EQUILIBRIUM MOR- PHOLOGY AND INTERFACIAL STRUCTURES OF PRICIPITATES IN DUPLEX STAINLESS STEEL BY ATOMISTIC SIMULATION[J]. 金属学报, 2014, 50(9): 1123-1127.
[12] CHEN Yulai, ZHANG Tairan, WANG Yide, LI Jingyuan. EFFECTS OF O, N AND Ni CONTENTS ON HOT PLASTICITY OF 0Cr25Ni7Mo4N DUPLEX STAINLESS STEEL[J]. 金属学报, 2014, 50(8): 905-912.
[13] XIANG Hongliang, GUO Peipei, LIU Dong. MICROSTRUCTURE AND ANTIBACTERIAL PROPERTIES OF Ag-BEARING DUPLEX STAINLESS STEEL[J]. 金属学报, 2014, 50(10): 1210-1216.
[14] BI Zongyue, YANG Jun, NIU Jing, ZHANG Jianxun. FRACTURE TOUGHNESS OF WELDED JOINTS OF X100 HIGH-STRENGTH PIPELINE STEEL[J]. 金属学报, 2013, 49(5): 576-582.
[15] XIANG Hongliang FAN Jinchun LIU Dong GUO Peipei. EFFECTS OF ANTIBACTERIAL AGING TREATMENT ON MICROSTRUCTURE AND PROPERTIES OF COPPER-CONTAINING DUPLEX STAINLESS STEEL
I. Microstructure and Evolution of Copper-Rich Phase
[J]. 金属学报, 2012, 48(9): 1081-1088.
No Suggested Reading articles found!