Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (3): 143-145    DOI:
Current Issue | Archive | Adv Search |
MSSBAUER STUDY ON MAGNETIC ANISOTROPY OF AMORPHOUS ALLOY Fe_(71)Ni_(10)B_(13)Si_4C_2
XU Zuxiong;MA Ruzhang;HAN Yongzhu University of Science and Technology Beijing Beijing Institute of Metallurgy
Cite this article: 

XU Zuxiong;MA Ruzhang;HAN Yongzhu University of Science and Technology Beijing Beijing Institute of Metallurgy. MSSBAUER STUDY ON MAGNETIC ANISOTROPY OF AMORPHOUS ALLOY Fe_(71)Ni_(10)B_(13)Si_4C_2. Acta Metall Sin, 1989, 25(3): 143-145.

Download:  PDF(262KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Magnetic anisotropies of the amorphous alloy Fe_(71)Ni_(10)B_(13)Si(14)C_2 annealed in mag-netic field have been studied using Mossbauer spectroscopy and X-ray diffraction. It is shownthat the distribution of moments in the annealed sample are determined by both stress-producedand thermomagnetic treatment-induced magnetic anisotropies.
Key words:  magnetic anisotropy      amorphous alloy      Mossbauer spectroscopy     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/143

1 Ok H N, Morrish A H. Phys Rev B, 1981; 23: 2257
2 Gonser U, Ackermann M, Wagner H G. J Magn Magn Mater. 1983, 31--34: 1605
3 Xu Zuxiong (徐祖雄), Ma Ruzhang (马如璋), Ping Jueyun (平爵云). Sci Sin. A, 1985; 28: 215
4 Schaafsma A S, Snijiders H, van der Woude F, Drijiver J W, Radelaar S. Phys Rev B, 1979; 20: 4423
[1] LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng. Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region[J]. 金属学报, 2022, 58(6): 807-815.
[2] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[3] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[4] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[5] LIU Riping, MA Mingzhen, ZHANG Xinyu. New Development of Research on Casting of Bulk Amorphous Alloys[J]. 金属学报, 2021, 57(4): 515-528.
[6] HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si. Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. 金属学报, 2021, 57(4): 542-552.
[7] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[8] HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo. Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems[J]. 金属学报, 2020, 56(6): 849-854.
[9] GENG Yaoxiang, WANG Yingmin. Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. 金属学报, 2020, 56(11): 1558-1568.
[10] XU Xiuyue, LI Yanhui, ZHANG Wei. Fabrication of Nanoporous PtRuFe by Dealloying Amorphous Fe(Pt, Ru)B Ribbons and Their Methanol Electrocatalytic Properties[J]. 金属学报, 2020, 56(10): 1393-1400.
[11] JIN Chenri, YANG Suyuan, DENG Xueyuan, WANG Yangwei, CHENG Xingwang. Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy[J]. 金属学报, 2019, 55(12): 1561-1568.
[12] HE Xianmei, TONG Liuniu, GAO Cheng, WANG Yichao. Effect of Nd Content on the Structure and Magnetic Properties of Si(111)/Cr/Nd-Co/Cr Thin Films Prepared by Magnetron Sputtering[J]. 金属学报, 2019, 55(10): 1349-1358.
[13] Xiaoqin MA, Qingfeng ZHAN, Jincai LI, Qingfang LIU, Baomin WANG, Runwei LI. Influence of Oblique Sputtering on Stripe Magnetic Domain Structure and Magnetic Anisotropy of CoFeB Thin Films[J]. 金属学报, 2018, 54(9): 1281-1288.
[14] Hongyang XU,Haibo KE,Huogen HUANG,Pei ZHANG,Pengguo ZHANG,Tianwei LIU. Nanoindentation Creep Behavior of U65Fe30Al5 Amorphous Alloy[J]. 金属学报, 2017, 53(7): 817-823.
[15] Dianguo MA,Yingmin WANG,Kunio YUBUTA,Yanhui LI,Wei ZHANG. Effect of Co Content on the Structure and Magnetic Properties of Melt-Spun Fe55-xCoxPt15B30 Alloys[J]. 金属学报, 2017, 53(5): 609-614.
No Suggested Reading articles found!