SOME CHARCTERISTICS OF MARTENSITE IN MEDIUM CARBON IRON ALLOY
LIU Yumen;HE Zhirong Xi'an Jiaotong University
Cite this article: 

LIU Yumen;HE Zhirong Xi'an Jiaotong University. SOME CHARCTERISTICS OF MARTENSITE IN MEDIUM CARBON IRON ALLOY. Acta Metall Sin, 1989, 25(2): 61-64.

Download:  PDF(544KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The morphology, subtructure and crystallography of martensite insteels 60 and 60Si2Mn have been Studied by means of optical and transmission elec-tron microscopy combined with B-M phenomenological crystallographic theory. Theaverage habit plane of martensite in medium carbon iron alloy is {225}_f. Experi-mental observations on habit plane and O-R are in agreement with the B-M theoryby using the Bain strain and lattice invariant shear on (100) [011]_f.
Key words:  Medium carbon steel      martensitic transformation      morphology      substruture     
Received:  18 February 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I2/61

1 徐祖耀.马氏体相变与马氏体,北京:科学出版社,1980:87,376
2 Wayman C. M. In: Cahn R W, Hoasen P eds., Physical Metallurgy, Elsevier Science Publishers BV, 1983: 1031
3 Wayman C M. Introduction to the Crystallography of Martensite Transformations, Macmillan, 1964
4 贺志荣.西安交通大学硕士论文,1986
5 Apple C A, Caron R N, Krauss G. Metall Trans, 1974; 5: 593
6 Porter D A. Phase Transformations in Metals and Alloys, Van Nostrard-Reinhold. New York, 1981; 390, 402
7 Dohmen U. Scr Metall, 1987; 21: 1029
[1] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[2] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[3] LI Min, LI Haoze, WANG Jijie, MA Yingche, LIU Kui. Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel[J]. 金属学报, 2022, 58(5): 637-648.
[4] LI Wei, JIA Xingqi, JIN Xuejun. Research Progress of Microstructure Control and Strengthening Mechanism of QPT Process Advanced Steel with High Strength and Toughness[J]. 金属学报, 2022, 58(4): 444-456.
[5] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[6] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[7] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[8] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[9] XIAO Fei, CHEN Hong, JIN Xuejun. Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy[J]. 金属学报, 2021, 57(1): 29-41.
[10] ZHANG Xinfang, YAN Longge. Regulating the Non-Metallic Inclusions by Pulsed Electric Current in Molten Metal[J]. 金属学报, 2020, 56(3): 257-277.
[11] LIU Haixia, CHEN Jinhao, CHEN Jie, LIU Guanglei. Characteristics of Waterjet Cavitation Erosion of 304 Stainless Steel After Corrosion in NaCl Solution[J]. 金属学报, 2020, 56(10): 1377-1385.
[12] SONG Xuexin, HUANG Songpeng, WANG Chuan, WANG Zhenyao. The Initial Corrosion Behavior of Carbon Steel Exposed to the Coastal-Industrial Atmosphere in Hongyanhe[J]. 金属学报, 2020, 56(10): 1355-1365.
[13] Wensheng XU, Wenzheng ZHANG. An Investigation of the Crystallography of Pearlites Nucleated on the Proeutectoid Cementite[J]. 金属学报, 2019, 55(4): 496-510.
[14] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[15] YANG Gaolin, LIN Xin, LU Xiangang. Crystallization Morphology and Evolution Mechanism of Laser Multiple Remelting of Zr55Cu30Al10Ni5 Metallic Glass[J]. 金属学报, 2019, 55(12): 1544-1550.
No Suggested Reading articles found!