DYNAMICS OF PRECIPITATION AND TRANSFORMATION OF CARBIDES IN A Ni-BASE SUPERALLOY
HUANG Qianyao;SHI Yanyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

HUANG Qianyao;SHI Yanyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. DYNAMICS OF PRECIPITATION AND TRANSFORMATION OF CARBIDES IN A Ni-BASE SUPERALLOY. Acta Metall Sin, 1988, 24(6): 399-403.

Download:  PDF(414KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The quantitative analytical method connecting the electrolyticextraction to X-ray diffraction analysis to determine the carbides and TCP in a Ni-base superalloy was developed. The alteration of decomposition of MC and precipi-tation of M_(23) C_6 and M_6 C with hot-exposure time under 850—1000℃ is shown ashyperbolic pattern. The elemental constitution of M_(23) C_6 changes continuously underhot exposure, (Cr_(0.67)Mo_(0.13)Ni_(0.13)Co_(0.07))_(23)C_6 precipitates from the beginning and (Cr_(0.88)Mo_(0.07)Ni_(0.03)Co_(0.02))_(23)C_6 On the end with the contents in increasing Cr and decreasingMo, Ni and Co. The higher the hot exposure temperature, the faster the final con-stitution of M_(23)C_6 may be easily achieved.
Key words:  Ni-base superalloy      carbide      hot exposure      electrolytic extraction      X-ray diffraction analysis     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/399

1 Collins H E, Quigg R J. ASM Trans Q, 1968; 61 (1) : 139
2 Collins H E. ASM Trans Q, 1969; 62 (1) : 82
3 Sims C T. In: Sims C T, Hagel W C et al. eds, The Superalloys, New York: Wiley, 1972: 259
[1] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[2] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[3] HE Shuwen, WANG Minghua, BAI Qin, XIA Shuang, ZHOU Bangxin. Effect of TaC Content on Microstructure and Mechanical Properties of WC-TiC-TaC-Co Cemented Carbide[J]. 金属学报, 2020, 56(7): 1015-1024.
[4] YANG Ke,LIANG Ye,YAN Wei,SHAN Yiyin. Preferential Distribution of Boron and its Effect on Microstructure and Mechanical Properties of (9~12)%Cr Martensitic Heat Resistant Steels[J]. 金属学报, 2020, 56(1): 53-65.
[5] LI Jiarong,XIE Hongji,HAN Mei,LIU Shizhong. High Cycle Fatigue Behavior of Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1195-1203.
[6] Futao DONG,Fei XUE,Yaqiang TIAN,Liansheng CHEN,Linxiu DU,Xianghua LIU. Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel[J]. 金属学报, 2019, 55(6): 792-800.
[7] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[8] Tao ZHANG, Wei YAN, Zhuoming XIE, Shu MIAO, Junfeng YANG, Xianping WANG, Qianfeng FANG, Changsong LIU. Recent Progress of Oxide/Carbide Dispersion Strengthened W-Based Materials[J]. 金属学报, 2018, 54(6): 831-843.
[9] Xirong LIU, Kai ZHANG, Shuang XIA, Wenqing LIU, Hui LI. Effects of Triple Junction and Grain Boundary Characters on the Morphology of Carbide Precipitation in Alloy 690[J]. 金属学报, 2018, 54(3): 404-410.
[10] Shenghu CHEN, Lijian RONG. Microstructure Evolution During Solution Treatment and Its Effects on the Properties of Ni-Fe-Cr Alloy[J]. 金属学报, 2018, 54(3): 385-392.
[11] Yubin DU, Xiaofeng HU, Haichang JIANG, Desheng YAN, Lijian RONG. Effect of Tempering Time on Carbide Evolution and Mechanical Properties in a Fe-Cr-Ni-Mo High-Strength Steel[J]. 金属学报, 2018, 54(1): 11-20.
[12] Bo CHEN, Xianchao HAO, Yingche MA, Xiangdong CHA, Kui LIU. Effects of Nitrogen Addition on Microstructure and Grain Boundary Microchemistry of Inconel Alloy 690[J]. 金属学报, 2017, 53(8): 983-990.
[13] Dawei WANG,Shichao XIU. Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint[J]. 金属学报, 2017, 53(5): 567-574.
[14] Dexin MA, Fu WANG, Xuhui WEN, Dejian SUN, Lin LIU. Influence of MC Carbides on the Formation of γ/γ′ Eutectics in Single Crystal Superalloy CM247LC[J]. 金属学报, 2017, 53(12): 1603-1610.
[15] Yingche MA,Shuo LI,Xianchao HAO,Xiangdong ZHA,Ming GAO,Kui LIU. RESEARCH ON THE CARBIDE PRECIPITATION AND CHROMIUM DEPLETION IN THE GRAIN BOUNDARY OF ALLOY 690 CONTAINING DIFFERENT CONTENTS OF NITROGEN[J]. 金属学报, 2016, 52(8): 980-986.
No Suggested Reading articles found!