| DIFFUSION REACTIONS BETWEEN Cu AND NbTi |
| XU Leying;WANG Wenbin;ZHUANG Yuzhi Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
XU Leying;WANG Wenbin;ZHUANG Yuzhi Institute of Metal Research; Academia Sinica; Shenyang. DIFFUSION REACTIONS BETWEEN Cu AND NbTi. Acta Metall Sin, 1988, 24(4): 335-341.
|
|
|
Abstract Diffusion reactions of superconducting composite NbTi/Cu, diffusioncouple Ti/Cu and Nb/Cu have been studied by means of EPMA. The results indica-te that the initial interface state of the composite NbTi/Cu significantly affect theforming process of intermetallic compounds at the interface, In comparision with themetallurgical binding composite, the intermetallic compounds forms at a higher tem-perature in mechanical binding one. Therefore, the mechanical binding process isbeneficial to the production of NbTi/Cu superconducting composite. No intermetallic compounds have been observed in Nb/Cu system. The morphol-ogy of intermetallic phases and the sequence in which they form in Ti/Cu systemare somewhat different to that in NbTi/Cu. The relationship between the thicknessof compound layer and anealing time obeys the rule of y~(1.5)--t.
|
|
Received: 18 April 1988
|
1 Ishibashi K, Wake M, Kobayashi M, Katase A. Cryogenics, 1979; 19: 3 161 2 #12 3 王文斌,徐乐英.辽宁冶金,1984;2:46 4 何寿安译.金属与合金中的扩散,北京:科学出版社,1958:80 5 Kaufman L, Bernstein H. In: Iaffee R I, Promise N E eds., The Science, Technology and Application of Ti, Pergamon Press, 1970: 361 6 Kubaschewski O, Alcock C B. Metyllurgical Thermochemistry, 5th ed., Pergamon Press, 1979: 193 7 Hansen P M. Constitution of Binary Alloys, 2nd ed., New York: McGraw-Hill, 1958; 643 8 Shunk F A. Constitution of Binary Allogs, 2nd Supplement, New York: McGraw-Hill, 1969; 209 9 William G M. The HandBook of Binary Phase Diagrams, Vol. I, USA: General Electric Company, 1976 10 Giessen B C. Szymanshi D. J Appi Crystallogr, 1971; 4: 257 11 Elliott R P. Constitution of Binary Alloys, 1st Supplement, New York: McGraw-Hill, 1965: 387v |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|