Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (2): 199-203    DOI:
论文 Current Issue | Archive | Adv Search |
RADIATION DAMAGE OF ~(111)In NUCLEI RECOIL-IMPLANTED IN Ag BY TDPAC METHOD
NI Xinbo;SUN Chongwen;CHEN Wenbiao;LU Qingqian Shanghai Institute of Nuclear Research; Academia Sinica
Cite this article: 

NI Xinbo;SUN Chongwen;CHEN Wenbiao;LU Qingqian Shanghai Institute of Nuclear Research; Academia Sinica. RADIATION DAMAGE OF ~(111)In NUCLEI RECOIL-IMPLANTED IN Ag BY TDPAC METHOD. Acta Metall Sin, 1988, 24(2): 199-203.

Download:  PDF(418KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The radiation damage was studied on ~(111)In nuclei recoil implanted inAg following ~(109)Ag(α,2n)~(111)In reaction by TDPAC method. The Ag foils(20μm) wereirradiated with 30MeV α particles under room temperature, the particle dose ratebeing 4.2×10~(12)cm~(-2)s~(-1). The experimental results indicated that the radiation damagewas severe in Ag even at room temperature. An electric field gradient of 10~(18) V/cm~2which is due to the radiation damage has been put onto the ~(111)Cd probe. The cubic Ag lattice was destroyed and lots of vacancies and interstitials cre-ated in Ag by radiation. The divacancy trapping has been suggested and the laserannealing has been conducted.

Key words:  radiation damage      laser annealing      ~(111)In      time differential perturbation angle correlation (TDPAC)     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/199

1 Herzog P, Freitag K, Reuschenbach M, Walitzki H. Z Phys, 1980: A294: 13 2 倪新伯.扰动角关联及其应用.北京:原子能出版社,1985:6 3 Thome L, Bernas H. Hyperfine Interactions, 1978; 5: 361 4 Behar M, Steffen R M. Phys Rev C, 1973; 7(2) : 788. 5 Wodniecki P, Krolas K, Marszatek M. Hyperfine Interactions, 1981; 10: 721 6 Sternheimer R. Phys Rev. 1951; 84: 244/1952; 86: 316 7 Feiock F D, Johnson W R. Phys Rev, 1969; 187: 39
[1] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[2] LIU Yue, TANG Pengzheng, YANG Kunming, SHEN Yiming, WU Zhongguang, FAN Tongxiang. Research Progress on the Interface Design and Interface Response of Irradiation Resistant Metal-Based Nanostructured Materials[J]. 金属学报, 2021, 57(2): 150-170.
[3] LIANG Jinjie, GAO Ning, LI Yuhong. Interaction Between Interstitial Dislocation Loop and Micro-Crack in bcc Iron Investigated by Molecular Dynamics Method[J]. 金属学报, 2020, 56(9): 1286-1294.
[4] Yucheng WU. Research Progress in Irradiation Damage Behavior of Tungsten and Its Alloys for Nuclear Fusion Reactor[J]. 金属学报, 2019, 55(8): 939-950.
[5] HUANG Yuan KONG Deyue HE Fang WANG Yulin LIU Wenxi. PREPARATION OF Mo/Ag LAMINAR COMPOSITES BY USING IRRADIATION DAMAGE ALLOYING METHOD[J]. 金属学报, 2012, 48(10): 1253-1259.
[6] LU Zheng. RADIATION-NDUCED EMBRITTLEMENT AND LIFE EVALUATION OF REACTOR PRESSURE VESSELS[J]. 金属学报, 2011, 47(7): 777-783.
[7] HE Xinfu YANG Peng YANG Wen. MOLECULAR DYNAMICS SIMULATION OF MATRIX RADIATION DAMAGE IN Fe-Cu ALLOY[J]. 金属学报, 2011, 47(7): 954-957.
[8] SUN Chao TAN Jun YING Shihao LI Cong PENG Qian ZHAO Suqiong. PREDICTION OF CRITICAL TEMPERATURE FOR DELAYED HYDRIDE CRACKING IN IRRADIATED N18 ZIRCONIUM ALLOY[J]. 金属学报, 2010, 46(7): 805-809.
[9] HU Benfu; HKINOSHITA Hiroshi; SAKAGUCHI Kisiki; TAKAHASHI Heishichiro. Radiation Damage Behavior of Carbide in Long Term Aging Treatmented Low Activation Austenitic Fe-Cr-Mn Alloy[J]. 金属学报, 2006, 42(3): 234-238 .
[10] HU Benfu; TAKAHASHI; Heishichiro. Effects of Helium on Behavior of Point Defect Produced by Irradiation in Low Activation Fe-Cr-Mn(W,V) Alloys[J]. 金属学报, 2004, 40(9): 955-961 .
[11] SUN Jiguang;CHEN Chaoqing;ZHANG Xishun (General Research institute for Nonferrous Metals; Beijing 100088)TIAN Yan;SHAN Bingquan;PAN Qingchun (Central Iron & Steel Research institute; Beijing 100081). PROPERTY OF RESISTANCE TO IRRADIATION DAMAGE OF ODS FERRITIC ALLOYS[J]. 金属学报, 1998, 34(11): 1210-1216.
[12] WAN Farong; HUANG Xuejun; KONG Feng;CHU Wuyang;XIAO Jimei(University of Science and Technology Beijing); TAKAHASHI Heishichiro(Hokkaido University; Japan). BEHAVIOUR OF OXIDE DISPERSION STRENTHENED FERRITIC STEEL UNDER ELECTRON IRRADIATION[J]. 金属学报, 1994, 30(22): 448-452.
[13] WAN Farong;XIAO Jimei;YUAN Yi University of Science and Technology Beijing lecturer;Department of Material Physics;University of Science and Technology Beijing; Beijing 100083. MEASUREMENT OF VACANCY MIGRATION ENERGY BY ELECTRON IRRADIATION[J]. 金属学报, 1990, 26(2): 74-78.
No Suggested Reading articles found!