Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (2): 194-198    DOI:
Current Issue | Archive | Adv Search |
SEPARATION AND CONCENTRATION OF Kr AND Xe FROM HYDROGEN USING TiFe_(0.86)Mn_(0.1) ALLOY
YANG Minjie;CHEN Bingzhao Shanghai Institute of Metallurgy; Academia Sinica
Cite this article: 

YANG Minjie;CHEN Bingzhao Shanghai Institute of Metallurgy; Academia Sinica. SEPARATION AND CONCENTRATION OF Kr AND Xe FROM HYDROGEN USING TiFe_(0.86)Mn_(0.1) ALLOY. Acta Metall Sin, 1988, 24(2): 194-198.

Download:  PDF(321KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Separation and concentration processes of Kr and Xe from hydrogenusing TiFe_(0.86)Mn_(0.1) alloy have been investigated at different temperatures. The resultsshow that the relation betwecn the concentration of Kr and Xe and the amountof desorpted hydrogen at 300 K obeys the equation N=αe~(-bV).
Key words:  Ti-Fe-Mn alloy      Kr      Xe      hydrogen storage property     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/194

1 中国科学院上海冶金研究所.3. 5M~3储氢合金瓶的特性及其使用说明,1983
2 Wenzl H. Int Metall Rev, 1982. 17(3) : 140
3 Shinjiro Wakao. Function and Materials. 1983; 3(4) : 1
4 复旦大学化学系.物理化学下册,1978;187
5 桂光燕,傅继文.特种气体,1985;2:51
[1] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[2] ZHANG Jun,JIE Ziqi,HUANG Taiwen,YANG Wenchao,LIU Lin,FU Hengzhi. Research and Development of Equiaxed Grain Solidification and Forming Technology for Nickel-Based Cast Superalloys[J]. 金属学报, 2019, 55(9): 1145-1159.
[3] Sansan SHUAI, Xin LIN, Wuquan XIAO, Jianbo YU, Jiang WANG, Zhongming REN. Effect of Transverse Static Magnetic Field on Microstructure of Al-12%Si Alloys Fabricated by Powder-BlowAdditive Manufacturing[J]. 金属学报, 2018, 54(6): 918-926.
[4] Yuan HOU, Zhongming REN, Jiang WANG, Zhenqiang ZHANG, Xia LI. Effect of Longitudinal Static Magnetic Field on the Columnar to Equiaxed Transition in Directionally Solidified GCr15 Bearing Steel[J]. 金属学报, 2018, 54(5): 801-808.
[5] Yongyong GONG, Shumin CHENG, Yuyi ZHONG, Yunhu ZHANG, Qijie ZHAI. The Solidification Technology of Pulsed Magneto Oscillation[J]. 金属学报, 2018, 54(5): 757-765.
[6] Jianbo YU, Yuan HOU, Chao ZHANG, Zhibin YANG, Jiang WANG, Zhongming REN. Effect of High Magnetic Field on the Microstructure in Directionally Solidified Co-Al-W Alloy[J]. 金属学报, 2017, 53(12): 1620-1626.
[7] Yuan SUN,Jide LIU,Xingyu HOU,Guanglei WANG,Jinxia YANG,Tao JIN,Yizhou ZHOU. MICROSTRUCTURE EVOLUTION AND INTERFACIAL FORMATION MECHANISM OF WIDE GAP BRAZING OF DD5 SINGLE CRYSTAL SUPERALLOY[J]. 金属学报, 2016, 52(7): 875-882.
[8] Huidong WU,Chi ZHANG,Wenbo LIU,Zhigang YANG. SIMULATION OF GROWTH KINETICS OF PRO-EUTECTOID FERRITE USING MIXED CONTROL MODEL WITH CONSIDERATION OF DISLOCATION INTERACTION[J]. 金属学报, 2015, 51(9): 1136-1144.
[9] HUANG Hefei, LI Jianjian, LIU Renduo, CHEN Huaican, YAN Long. TEMPERATURE EFFECT OF Xe ION IRRADIATION TO 316 AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2014, 50(10): 1189-1194.
[10] HANG Chunjin, TIAN Yanhong,ZHAO Xin, WANG Chunqing. RESEARCH ON MICROSTRUCTURE OF Pb-FREE BGA SOLDER JOINT ASSEMBLED WITH Sn-Pb SOLDER DURING ISOTHERMAL AGING[J]. 金属学报, 2013, 49(7): 831-837.
[11] LIU Jing LUO Xinghong HU Xiaoqiang LIU Shi. EFFECT OF Ti AND Nb MICRO–ALLOYING ON THE MICROSTRUCTURE OF THE ULTRA–PURIFIED 11%Cr FERRITE STAINLESS STEELS[J]. 金属学报, 2011, 47(6): 688-696.
[12] KANG Jinwu NIE Gang YU Hailiang LONG Haimin HAO Xiaokun HUANG Tianyou HU Yongyi. THREE DIMENSIONAL DYNAMICAL MEASUREMENT OF DISTORTION OF HEAVY STEEL CASTINGS DURING HEAT TREATMENT PROCESS[J]. 金属学报, 2011, 47(5): 535-539.
[13] LIU Zhiyuan YANG Zhigang LI Zhaodong LIU Zhenqing ZHANG Chi. SIMULATION OF LEDGEWISE GROWTH KINETICS OF PROEUTECTIOD FERRITE UNDER INTERFACIAL REACTION–DIFFUSION MIXED CONTROL MODEL[J]. 金属学报, 2010, 46(4): 390-395.
[14] CONG Baoqiang QI Bojin ZHOU Xingguo LUO Jun. INFLUENCES OF ULTRASONIC PULSE SQUARE-WAVE CURRENT PARAMETERS ON MICROSTRUCTURES AND MECHANICAL PROPERTIES OF 2219 ALUMINUM ALLOY WELD JOINTS[J]. 金属学报, 2009, 45(9): 1057-1062.
[15] XU Xiujie DENG Anyuan WANG Engang ZHANG Lintao ZHANG Yongjie HE Jicheng. EFFECT MECHANISM OF HIGH FREQUENCY ELECTROMAGNETIC FIELD ON THE SURFACE QUALITY AND EQUIAXED CRYSTAL RATIO OF 15CrMo BILLET[J]. 金属学报, 2009, 45(11): 1330-1335.
No Suggested Reading articles found!