Acta Metall Sin  2011, Vol. 47 Issue (7): 777-783    DOI: 10.3724/SP.J.1037.2011.00265
论文 Current Issue | Archive | Adv Search |
RADIATION-NDUCED EMBRITTLEMENT AND LIFE EVALUATION OF REACTOR PRESSURE VESSELS
LU Zheng
Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819
Cite this article: 

LU Zheng. RADIATION-NDUCED EMBRITTLEMENT AND LIFE EVALUATION OF REACTOR PRESSURE VESSELS. Acta Metall Sin, 2011, 47(7): 777-783.

Download:  PDF(925KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Neutron irradiation can lead to the embrittlement and the shift of ductile-brittle transition temperature (DBTT) of the reactor pressure vessel (RPV) steels, which is the potential threat to the safe operation of reactors. Surveillance program for RPVs, irradiation damage and embrittlement of RPV steels and safe evaluation of RPVs were reviewed in this paper.
Key words:  reactor pressure vessel      irradiation damage      DBTT shift      life evaluation     
Received:  25 April 2011     
Fund: 

Supported by National Natural Science Foundation of China (Nos.50971033 and 91026013), National Basic Research Program of China (No.2011CB610405), Fundamental Research Funds for the Central Universities (No.N100402001) and Program for New Century Excellent Talents in University (No.NCET-10-0302)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2011.00265     OR     https://www.ams.org.cn/EN/Y2011/V47/I7/777

[1] Odette G R, Lucas G E. JOM, 2001; 53: 18

[2] Little E A. Proc EUROMAT 96, Conf Materials and Nuclear Power, London: Institute of Materials, 1996: 29

[3] Nanstad R K, Sokolov M A, McCabe D E. J ASTM Int, 2008; 5: JAI101346

[4] Steele L E. In: Steele L E, ed., Status of USA Nuclear Reactor Pressure Vessel Surveillance for Radiation Effects, ASTM STP 784, Philadelphia, PA: American Society for Testing and Materials, 1983: 277

[5] Wallin K. Eng Fract Mech, 2002; 69: 451

[6] Little E A. Proc Conf Dimensional Stability and Mechanical Behavior of Irradiated Metals and Alloys, London: BNES, 1984: 141

[7] Guionnet C, Robin Y, Flavier C, Lefort A, Gros D, Perdreau R. In: Kramer D, Brager H R, Perrin J S, eds., Effects of Radiation on Materials: Proceedings of the Tenth International Symposium, ASTM STP 725, Philadelphia, PA: American Society for Testing and Materials, 1981: 20

[8] Monzen R, Iguchi M, Jenkins M L. Philos Mag Lett, 2000; 80: 137

[9] Phythian W J, English C A. J Nucl Mater, 1993; 205: 162

[10] Miller M K, Russell K F, Sokolov M A, Nanstad R K. J Nucl Mater, 2003; 320: 177

[11] Faulkner R G, Lu Z, Ellis D, Williams T J. J ASTM Int, 2005; 2: 285

[12] Buswell J T, Little E A, Sinclair R N. Nucl Energy, 1998; 37: 387

[13] Schilling W, Ullmaier H. In: Cahn R W, eds., Materials Science and Technology: Nuclear Materials, Vol.10B, Germany: Wiley–VCH, 1994: 179

[14] Domain C, Becquart C S, Malerba L. J Nucl Mater, 2004; 335: 121

[15] Jenkins M L, Kirk M A. Characterisation of Radiation Damage by Transmission Electron Microscopy. Bristol and Philadelphia: IOP Publishing, 2001: 126

[16] Little E A, Harries D R. Met Sci, 1970; 4: 188

[17] English C A, Ortner S R, Gage G, Server W L, Rosinski S T. In: Rosinski S T, Grossbeck M L, Allen T R, Kumar A S, eds., Effects of Radiation on Materials: 20th International Symposium, ASTM STP 1405, West Conshohocken, PA: American Society for Testing and Materials, 2001: 151

[18] Bischler P J E, Wild R K. In: Gelles D S, Nanstad R K, Kumar A S, Little E A, eds., Effects of Radiation on Materials: 17th International Symposium, ASTM STP 1270, West Conshohocken, PA: American Society for Testing and Materials, 1996: 260

[19] Faulkner R G, Jones R B, Lu Z, Flewitt P E J. Philos Mag, 2005; 85: 2065

[20] Pechenkin V A, Konobeev Y V, Stepanov I A, Nikolaev Y A. In: Grossbeck M L, Allen T R, Lott R G, Kumar A S, eds., Effects of Radiation on Materials: 21st International Symposium, ASTM STP 1447, West Conshohocken, PA: American Society for Testing and Materials, 2004: 138

[21] Lu Z, Faulkner R G, Flewitt P E J. Mater Sci Eng, 2006; A437: 306

[22] Lu Z, Faulkner R G, Sakaguchi N, Kinoshita H, Takahashi H J, Flewitt P E. J Nucl Mater, 2006; 351: 155

[23] Brillaud C, Hedin F, Houssin B. In: Garner F A, Henager C H, Igata N, eds., Influence of Radiation on Material Properties: 13th International Symposium, ASTM STP 956, Philadelphia, PA: American Society for Testing and Materials, 1987: 420

[24] Petrequin P. A Review of Formulas for Predicting Irradiation Embrittlement of Reactors Vessel Materials, AMES Report No.6, 1996: 13

[25] Odette G R, Mader E V, Lucas G E, Phythian W J, English C A. In: Kumar A S, Gelles D S, Nanstad R K, Little E A, eds., Effects of Radiation on Materials: 16th International Symposium, ASTM STP 1175, Philadelphia, PA: American Society for Testing and Materials, 1993: 373

[26] Odette G R, Yamamoto R T, Klingensmith R D. Philos Mag, 2005; 85: 779

[27] Miller M K, Russell K F. J Nucl Mater, 2007; 37: 145

[28] Odette G R, Wirth B D. J Nucl Mater, 1998; 251: 157
[1] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[2] Yucheng WU. Research Progress in Irradiation Damage Behavior of Tungsten and Its Alloys for Nuclear Fusion Reactor[J]. 金属学报, 2019, 55(8): 939-950.
[3] Tianci ZHANG, Haitao WANG, Zhengcao LI, Henk SCHUT, Zhengming ZHANG, Ming HE, Yuliang SUN. Positron Annihilation Investigation of Embrittlement Behavior in Chinese RPV Steels after Fe-Ion Irradiation[J]. 金属学报, 2018, 54(4): 512-518.
[4] LI Zhengcao, CHEN Liang. IRRADIATION EMBRITTLEMENT MECHANISMS AND RELEVANT INFLUENCE FACTORS OF NUCLEAR REACTOR PRESSURE VESSEL STEELS[J]. 金属学报, 2014, 50(11): 1285-1293.
[5] XU Gang CAI Linling FENG Liu ZHOU Bangxin LIU Wenqing WANG Junan. SEGREGATION OF ATOMS ON THE INTERFACES IN THE RPV MODEL STEEL STUDIED BY APT[J]. 金属学报, 2012, 48(7): 789-796.
[6] XU Gang, CAI Linling, FENG Liu, ZHOU Bangxin,WANG Jun'an,ZHANG Haisheng. EFFECT OF THE PRECIPITATION OF Cu-RICH CLUSTERS ON THE DBTT OF RPV SIMULATED STEEL[J]. 金属学报, 2012, 48(6): 753-758.
[7] XU Gang, CAI Linling, FENG Liu, ZHOU Bangxin,LIU Wenqing, WANG Jun'an. STUDY ON THE PRECIPITATION OF Cu-RICH CLUSTERS IN THE RPV MODEL STEEL BY APT[J]. 金属学报, 2012, 48(4): 407-413.
[8] HUANG Yuan KONG Deyue HE Fang WANG Yulin LIU Wenxi. PREPARATION OF Mo/Ag LAMINAR COMPOSITES BY USING IRRADIATION DAMAGE ALLOYING METHOD[J]. 金属学报, 2012, 48(10): 1253-1259.
[9] ZHONG Weihua TONG Zhenfeng ZHANG Changyi QIAO Jiansheng YANG Wen. SMALL PUNCH TESTING OF THE EFFECT OF IRRADIATION ON MECHANICAL PROPERTY OF RPV STEEL[J]. 金属学报, 2011, 47(9): 1205-1209.
[10] XU Gang CHU Dafeng CAI Linling ZHOU Bangxin WANG Wei PENG Jianchao. INVESTIGATION ON THE PRECIPITATION AND STRUCTURAL EVOLUTION OF Cu-RICH NANOPHASE IN RPV MODEL STEEL[J]. 金属学报, 2011, 47(7): 905-911.
[11] SUN Chao TAN Jun YING Shihao LI Cong PENG Qian ZHAO Suqiong. PREDICTION OF CRITICAL TEMPERATURE FOR DELAYED HYDRIDE CRACKING IN IRRADIATED N18 ZIRCONIUM ALLOY[J]. 金属学报, 2010, 46(7): 805-809.
[12] HU Benfu; HKINOSHITA Hiroshi; SAKAGUCHI Kisiki; TAKAHASHI Heishichiro. Radiation Damage Behavior of Carbide in Long Term Aging Treatmented Low Activation Austenitic Fe-Cr-Mn Alloy[J]. 金属学报, 2006, 42(3): 234-238 .
[13] HU Benfu; TAKAHASHI; Heishichiro. Effects of Helium on Behavior of Point Defect Produced by Irradiation in Low Activation Fe-Cr-Mn(W,V) Alloys[J]. 金属学报, 2004, 40(9): 955-961 .
[14] SUN Jiguang;CHEN Chaoqing;ZHANG Xishun (General Research institute for Nonferrous Metals; Beijing 100088)TIAN Yan;SHAN Bingquan;PAN Qingchun (Central Iron & Steel Research institute; Beijing 100081). PROPERTY OF RESISTANCE TO IRRADIATION DAMAGE OF ODS FERRITIC ALLOYS[J]. 金属学报, 1998, 34(11): 1210-1216.
[15] WAN Farong; HUANG Xuejun; KONG Feng;CHU Wuyang;XIAO Jimei(University of Science and Technology Beijing); TAKAHASHI Heishichiro(Hokkaido University; Japan). BEHAVIOUR OF OXIDE DISPERSION STRENTHENED FERRITIC STEEL UNDER ELECTRON IRRADIATION[J]. 金属学报, 1994, 30(22): 448-452.
No Suggested Reading articles found!