EFFECTS OF P CONTENT ON (LAVES+γ) EUTECTIC REACTION DURING INCONEL 706 ALLOY SOLIDIFICATION
XIN Xin1, 2), HUANG Aihua3), QI Feng2), ZHANG Weihong2), LIU Fang2) ,YANG Hongcai1), SUN Wenru2) , HU Zhuangqi2)
1) School of Materials and Metallurgy, Northeastern University, Shenyang 110819
2) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
3) Shenyang Liming Aero--Engine Group Corporation, Shenyang 110043
Cite this article:
XIN Xin HUANG Aihua QI Feng ZHANG Weihong LIU Fang YANG Hongcai SUN Wenru HU Zhuangqi . EFFECTS OF P CONTENT ON (LAVES+γ) EUTECTIC REACTION DURING INCONEL 706 ALLOY SOLIDIFICATION. Acta Metall Sin, 2010, 46(7): 873-878.
The effects of P on elemental segregation and as-cast microstructure in Inconel 706 alloy were investigated in this paper. The results showed that P was markedly enriched in residual liquid and enhanced the segregation of Nb and Ti, which promoted the precipitation of Nb-enriched Laves phase and Ti-enriched η-Ni3Ti phase. In the as-cast alloy doped with 0.004% P (mass fraction), fine (Laves+γ) eutectic and needle like $\eta$ phase were formed in interdendritic region. As the P dopant was higher than 0.016%, blocky Laves phase was formed and lath η particles were precipitated among Laves particles. Moreover, with P increasing from 0.004\% to 0.016%, the incipient melting-point was found to drop from 1170-1180 ℃ to 1160-1170 ℃. In high P-doped alloys, the enrichment of P in the residual liquid was believed to hinder the solidification of γ phase, as a result, the final solidification temperature was found to be decreased and the solidification was terminated by the solidification of γ phase prior to the formation of P-bearing Laves phase rather than forming the (Laves+γ) eutectic.
[1] Schilke P W, Pepe J J, Schwant R C. In: Loria E A ed., Superalloys 718,625,706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1994: 1
[2] Schilke P W, Schwant R C. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 2001: 25
[3] Long Z D. Mater Rev, 1995; 5: 14
(龙正东. 材料导报, 1995; 5: 14)
[4] Hu Z Q, Sun W R, Guo S R, Lu D Z. Chin J Nonferrous Met, 2001; 11: 947
(胡壮麒, 孙文儒, 郭守仁, 卢德忠. 中国有色金属学报, 2001; 11: 947)
[5] Sun WR, Guo S R, Guo J T, Lu D Z, Hu Z Q. Acta Metall Sin, 1995; 31: 346
(孙文儒, 郭守仁, 郭建亭, 卢德忠, 胡壮麒. 金属学报, 1995; 31: 346)
[6] Sun WR, Guo S R, Lee J H, Park P K, Yoo Y S, choe S J, Hu Z Q. Mater Sci Eng, 1998; A247: 173
[7] Cao W D, Kennedy R L. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1994: 463
[8] Song H W. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 1999
(宋洪伟. 中国科学院金属研究所博士论文, 沈阳, 1999)
[9] Huang L F. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2007
(黄历锋. 中国科学院金属研究所博士论文, 沈阳, 2007)
[10] Yang S L. PhD Thesis, Northeastern University, Shenyang, 2006
(杨树林. 东北大学博士论文, 沈阳, 2006)
[11] Yang S L, Sun W R, Wang J X, Wang K L, Guo S R, Hu Z Q. Acta Metall Sin, 2009; 45: 815
(杨树林, 孙文儒, 王健熙, 王克亮, 郭守仁, 胡壮麒. 金属学报, 2009; 45: 815)
[12] Fesland J P, Petit P. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS– AIME, 1994: 229
[13] Meng X N, Sun W R, Guo S R, Lu D Z, Li N. Acta Metall Sin, 2004; 40: 613
(孟晓娜, 孙文儒, 郭守仁, 卢德忠, 李 娜. 金属学报, 2004; 40: 613)
[14] Chen C, Thompson R G, Davis S W. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1991: 81