| Fe-Nb合金在600-800℃,0.1MPa纯氧中的氧化 |
| 牛焱;吴维 |
| 中国科学院金属腐蚀与防护研究所;金属腐蚀与防护国家重点实验室 |
|
| OXIDATION OF Fe-Nb ALLOYS UNDER 0.1 Mpa PURE OXYGEN AT 600─800℃ |
| NIU Yan; WU Weitao; FGESMUNDO; FC.RIZZO;(State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 1 100015 )(Istituto di Chimica; Facolta di Ingegneria; Universita' di Genova; Fiera del Mare;Pad. D; 16129 Genova; Italy )(Departamento de Ciencia dos Materiais e Metalurgia; Pontificia Universidade Catolica do Rio de Janeiro; Caixa Postal 38008; 22453-900; RJ; Brazil )(Manuscript received 1995-05- 19; in revised form 1 995-09-08) |
引用本文:
牛焱;吴维. Fe-Nb合金在600-800℃,0.1MPa纯氧中的氧化[J]. 金属学报, 1996, 32(3): 294-302.
,
.
OXIDATION OF Fe-Nb ALLOYS UNDER 0.1 Mpa PURE OXYGEN AT 600─800℃[J]. Acta Metall Sin, 1996, 32(3): 294-302.
| 1NiuY,GesmundoF,VianiF.CorrosSci,1994;36:8832CastroM,NiuY,RizzoF,GesmundoF.OxidMet,1995;43:5613NiuY,GesmundoF,VianiF.CorrosSci,inprint4SvedbergRC.in:ForoulisZA,PettitFS,Eds,PropertiesofHighTemperatureAlloys,Princeton,NJ:TheElectrochemSoc,1977.3315RappRA,Corrosion,1965;21:3826GesmundoF,NiuY,VianiF,KizzoF.OxidMet,tobepublished7GesmundoF,NiuY,VianiF.OxidMet.1995;43:3798GesmundoF,VianiF,NiuY,DouglassDL.OxidMet,1994;42:4659GesmundoF,VianiF.OxidMet,1986;25:26910GesmundoF,VianiF,NiuY.OxidMet,1994;42:40911MrowecS.GasCorrosionofMetals,Washington:NationalBureauofstandards,197812BirchenallCE.In:DouglassDL,ed,OxidationofMetalsandAlloys,AmericanSoc.forMetals,MetalsPark,1971:17713PaidassiJ.In:BenardJ,ed,L′OxydationdesMetaux,Paris:Gauthier-Villars,1964,vol.Ⅱ,p.13x |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|