| 代位合金元素原子在Fe_3Al金属间化合物亚点阵占位的中子衍射研究 |
| 杨王玥;盛丽珍;孙祖庆;黄原定;毛卫民;张百生;叶春堂 |
| 北京科技大学;中国原子能科学院 |
|
| NEUTRON DIFFRACTION STUDY ON SITE OCCUPATION OF SUBSTITUTIONAL ELEMENTS AT SUBLATTICE IN Fe_3Al INTERMETALLICS |
| YANG Wangyue; SHENG Lizhen;SUN Zuqing; HUANG Yuanding; MAO Weimin (University of Science and Technology Beijing; Beijing 100083); ZHANG Baisheng; YE Chuntang (China Institute of Atomic Energy; Beijing 102413)(Manuscript received 1995-11-10; in revised form 1996-04-05) |
引用本文:
杨王玥;盛丽珍;孙祖庆;黄原定;毛卫民;张百生;叶春堂. 代位合金元素原子在Fe_3Al金属间化合物亚点阵占位的中子衍射研究[J]. 金属学报, 1996, 32(8): 799-804.
,
,
,
,
,
,
.
NEUTRON DIFFRACTION STUDY ON SITE OCCUPATION OF SUBSTITUTIONAL ELEMENTS AT SUBLATTICE IN Fe_3Al INTERMETALLICS[J]. Acta Metall Sin, 1996, 32(8): 799-804.
| 1McKameyCG,DeVanJH,TortorelliPF,SikkaVK.JMaterRes,1991;6:17792MckameyCG,HortonJA,LiuCT,JMaterRes,1989;4:11563SunZQ,HuangYD,YangWY,ChenGL.MaterResSocSympProc,1993;288:8854孙祖庆,黄原定,杨王,毛卫民,陈国良,金属学报,1993;29:A3545杨王,盛丽珍,徐峰,黄原定,孙祖庆.北京科技大学学报,1996;18:2496RietveldHM.JApplCrystallogr,1969;2:657BaconGE著,谈洪,乐英译.中子衍射.北京:科学出版社,1980:3838杨王,盛丽珍,黄原定,孙祖庆,张百生.材料研究学报,1996;(8):待发表9杨王,盛丽珍,黄原定,毛卫民,孙祖庆.中国有色金属学报,1996;4(6):待发表 |
|