| 热轧变形对快凝Al-Fe-V-Si粉热挤合金断裂行为的影响 |
| 曾欲晓;黎文献;李松瑞;肖于德;陈伶晖 |
| 中南工业大学 |
|
| INFLUENCE OF HOT ROLLING ON FRACTURE BEHAVIOUR OF Al-Fe-V-Si ALLOY PREPARED BY HOT EXTRUSION OF RAPIDLY SOLIDIFIED POWDERS |
| ZENG Yuxiao; LI Wenxian; LI Songrui; XIAO Yude; CHEN Linghui (Central South University of Technology; Changsha 410083)(Manuscript received 1995-10-05; in revised form 1996-03-18) |
引用本文:
曾欲晓;黎文献;李松瑞;肖于德;陈伶晖. 热轧变形对快凝Al-Fe-V-Si粉热挤合金断裂行为的影响[J]. 金属学报, 1996, 32(8): 839-844.
,
,
,
,
.
INFLUENCE OF HOT ROLLING ON FRACTURE BEHAVIOUR OF Al-Fe-V-Si ALLOY PREPARED BY HOT EXTRUSION OF RAPIDLY SOLIDIFIED POWDERS[J]. Acta Metall Sin, 1996, 32(8): 839-844.
| 1SkinnerDJ,ByeRL,RayhouldD.ScrMetall,1986;20:8672FrnakRE,HawkJA.ScrMetall,1989;23:1133SkinnerDJ.In:KimYW,GriffithWMeds.,DispersionStrengthenedAluminumAlloys,MMMS,1988:1814MitraS.ScrMetallMater,1992;27:5215LeeS,LeeDY,KimNJ.MaterSciEng,1991;A143:336LeeJC,LeeS,LeeDY.MetallTrans,1991;22A:8537HariprasadS.MetallMaterTrans,1994,25A:10058ChanKS.MetallTrans,1989;20A1159ChanKS.MetallTrans,1989;20A:2337T |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|