| 连铸中间包内钢液流动与传热耦合过程的计算机模拟 |
| 朱苗勇 |
| 东北大学;沈阳;110006 |
|
| NUMERICAL SIMULATION OF THE COUPLED MOLTEN STEEL FLOW AND HEAT TRANSFER IN CONTINUOUS CASTING TUNDISHES |
| ZHU Miaoyong(Northeastern Universily; Shenyang 110006) |
引用本文:
朱苗勇. 连铸中间包内钢液流动与传热耦合过程的计算机模拟[J]. 金属学报, 1997, 33(9): 933-938.
.
NUMERICAL SIMULATION OF THE COUPLED MOLTEN STEEL FLOW AND HEAT TRANSFER IN CONTINUOUS CASTING TUNDISHES[J]. Acta Metall Sin, 1997, 33(9): 933-938.
1Lai K Y M,Salcudean M,Tanaka S Guthrie R I L Metall Trans,1986;17B:449 2Szekely J,EI-Kaddah N.Steelmaking Proc,1986;69:761 3He Y,Sahai Y.Metall Trans,1987;18B:81 4Tacke K H,Ludwig J C Steel Res ,1987;58:262 5Sinha A K,Sahai Y.ISIJ Int,1993;33:556 6Chakraborty S Sahai Y.Ironmak Steelmak 1992;19:479 7Joo S, Han J W,Guthrie R I L.Metall Trans, 1993 24B:767 8朱苗勇,郁夫金属学报,1997待发表工作 9Launder B E Splading D B.Comput Meth Appl Mech Eng,1974;3:269 10朱苗勇.东北大学博士学位论文,199 |
|