| 铝合金薄板搅拌摩擦焊接残余变形的数值分析 |
| 鄢东洋1;史清宇1;吴爱萍1;Juergen Silvanus2;刘园1;张增磊1 |
1. 清华大学机械工程系; 北京 100084
2. European Aeronautic Defence and Space Company Innovation Works; Munich 81663; Germany |
|
| NUMERICAL ANALYSIS ON THE RESIDUAL DISTORTION OF Al ALLOY SHEET AFTER FRICTION STIR WELDING |
| YAN Dongyang 1; SHI Qingyu 1; WU Aiping 1; Juergen Silvanus 2; LIU Yuan 1; ZHANG Zenglei 1 |
1. Department of Mechanical Engineering; Tsinghua University; Beijing 100084
2. European Aeronautic Defence and Space Company Innovation Works; Munich 81663; Germany |
引用本文:
鄢东洋 史清宇 吴爱萍 Juergen Silvanus 刘园 张增磊. 铝合金薄板搅拌摩擦焊接残余变形的数值分析[J]. 金属学报, 2009, 45(2): 183-188.
,
,
,
,
,
.
NUMERICAL ANALYSIS ON THE RESIDUAL DISTORTION OF Al ALLOY SHEET AFTER FRICTION STIR WELDING[J]. Acta Metall Sin, 2009, 45(2): 183-188.
| [1] Thomas W M, Nicholas E D, Needham J C, Murch M G, Templesmith P, Dawes C J. Gr Br Pat Appl No. 9 125978.8, 1991
[2] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1
[3] Tang W, Guo X, McClure J C, Murr L E. J Mater Process Manuf Sci, 1998; 7(2): 163
[4] Staron P, Kocak M. In: David S A, Debroy T, Lippold J C, Smartt H B, Vitek J M eds., Proc 6th Int Conf on Trends in Welding Research, Pine Mountain: ASM International, 2003: 216
[5] Song M, Kovacevic R. J Eng Manuf, 2003; 217(1): 73
[6] Colegrove P A, Shercliff H R. Sci Technol Weld Join, 2003; 8: 360
[7] Chao Y J, Qi X, Tang W. Trans ASME, 2003; 125: 138
[8] Shi Q Y, Dickerson T L, Shercliff H R. Proc 4th Int Symp on Friction Stir Welding, TWI Center, Park City, USA, 2003 (CD–ROM)
[9] Li T, Shi Q Y, Li H K. Sci Technol Weld Join, 2007; 12: 664
[10] Price D A, Williams S W, Wescott A, Harrison C J C, Rezai A, Steuwer A, Peel M, Staron P, Kocak M. Sci Technol Weld Join, 2007; 12: 620
[11] Shi Q Y, Silvanus J, Liu Y, Yan D Y, Li H K. Sci Technol Weld Join, 2008; 13: 472
[12] Chai P, Luan G H, Guo D L, Li J, Trans Chin Weld Inst, 2005; 26(11): 79
(柴 鹏, 栾国红, 郭德伦, 李菊. 焊接学报, 2005; 26(11): 79)
[13] Grimvall G. Thermophysical Properties of Materials: Non Metallic Solids. New York: Elsevier, 1999: 243
[14] Parrott J E, Stuckes A D. Thermal Conductivity of Solids. London: Pion, 1975: 156
[15] Preston R V. PhD Thesis, Cambridge University, 2000
[16] Zhu X K, Chao Y J. J Mater Process Technol, 2004; 146: 263
[17] Li H K. Postdoctoral Report, Tsinghua University, Beijing, 2007
[18] Wu C S. Numerical Analysis for Heat Transfer in Welding Process. Harbin: Harbin Institute of Technology Press, 1990: 95
武传松. 焊接热过程数值分析. 哈尔滨: 哈尔滨工业出版社, 1990: 95)
[19] Shi Q Y, Dickerson T L, Shercliff H R. In: David S A, DebRoy T, Lippold J C, Smartt H B, Vitek J M eds., Proc 6th Int Conf on Trends in Welding Research, Pine Mountain: ASM International, 2003: 247
[20] Dickerson T L, Shi Q Y, Shercliff H R. Proc 4th Int Symp On Friction Stir Welding, TWI Center, Park City, USA, 2003 (CD–ROM)
[21] Vuyst T, Dealvise L D. Proc 5th Int Symp on Friction Stir Welding, TWI Center, Park City, USA, 2004 (CD–ROM)
[22] Buffa G, Hua J, Shivpuri R, Fratini L. Mater Sci Eng,2006; A419: 389 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|