| 氮含量对脉冲偏压电弧离子镀CNx薄膜结构与性能的影响 |
| 李红凯;林国强;董闯;闻立时 |
| 大连理工大学三束材料改性国家重点实验室 |
|
| EFFECT OF NITROGEN CONTENT ON THE MICROSTRUCTURE AND PROPERTIES OF CNx FILMS DEPOSITED BY PULSED BIAS |
| Hong-Kai LI;;;; |
引用本文:
李红凯; 林国强; 董闯; 闻立时 . 氮含量对脉冲偏压电弧离子镀CNx薄膜结构与性能的影响[J]. 金属学报, 2008, 44(8): 917-921 .
,
,
,
.
EFFECT OF NITROGEN CONTENT ON THE MICROSTRUCTURE AND PROPERTIES OF CNx FILMS DEPOSITED BY PULSED BIAS[J]. Acta Metall Sin, 2008, 44(8): 917-921 .
[1]Wang E G.Prog Mater Sci,1997;41:241 [2]Widlow I,Chung Y W.Int Mater Rev,2002;47:153 [3]Stephen M,Juan M M.Diamond Relat Mater,1999;8: 1809 [4]Martin P J,Bendavid A.Thin Solid Films,2001;394:1 [5]Lin G Q,Zhao Y H,Guo H M,Wang D Z,Dong C,Huang R F,Wen L S.J Vac Sci Technol,2004;22:1218 [6]Zhou Z M,Xia L F.Surf Coat Technol,2003;172:102 [7]Hammer P,Victoria N M,Alvarez F.J Vac Sci Technol, 2000;18:2277 [8]Tian X M,Adhikari S,Adhikary S,Uchida H,Umeno M, Soga T,Jimbo T.Diamond Relat Mater,2005;14:1839 [9]Shi J R.J Appl Phys,2006;99:1 [10]Hainsworth S V,Uhure N J.Int Mater Rev,2007;52:153 [11]Li L H,Wu Y Q,Cui X M,Zhang H Q,Zhang Y H,Xia L F,Chu P K.Acta Metall Sin,2004;40:220 (李刘合,武咏琴,崔旭明,张海泉,张彦华,夏立芳,朱剑豪.金属学报,2004;40:220) [12]Ferrari A C.Diamond Relat Mater,2002;11:1053 [13]Zou Y S,Wang W,Zheng J D,Sun C,Huang R F,Wen L S.Acta Metall Sin,2004;40:537 (邹友声,汪伟,郑静地,孙超,黄荣芳,闻立时.金属学报,2004;40:537) [14]Bai H L,Jiang E Y,Wu P,Wang Y,Wang C D.Acta Metall Sin,1999;35:762 (白海力,姜恩永,吴萍,王怡,王存达.金属学报,1999;35:762) [15]Robertson J.Mater Sci Eng,2002;R37:129 [16]Silva S R P,Robertson J,Amaratunga G A J,Rafferty B, Brown L M,Schwan J,Franceschini D F,Mariotto G.J Appl Phys,1997;81:2626 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|