| 微细铜粉250-400 ℃空气中的氧化行为 |
| 郭艳辉;张楠;陈纪忠 |
| 浙江大学化学工程与生物工程学系国家重点化学工程联合实验室 |
|
| Oxidation behavior of fine copper powder between 250-400℃ |
| Guo Yan-Hui;Nan Zhang;Jizhong Chen |
| 浙江大学 |
引用本文:
郭艳辉; 张楠; 陈纪忠 . 微细铜粉250-400 ℃空气中的氧化行为[J]. 金属学报, 2008, 44(7): 821-825 .
,
,
.
Oxidation behavior of fine copper powder between 250-400℃[J]. Acta Metall Sin, 2008, 44(7): 821-825 .
[1]Tu H L,Zhao G Q,Guo Q W.Nonferrous Metals- Metallurgy,Material,Reproduct and Environmental Pro- teetion.Beijing:Chemical Industry Press,2003:14 (屠海令,赵国权,郭青蔚.有色金属——冶金、材料、再生与环保.北京:化学工业出版社,2003:14) [2]Patil S,Salnkar S It,Patti P P.Appl Surf Sci,2004;225: 204 [3]Han Z,Lu L,Zhang H W,Yang Z Q,Wang F H,Lu K. Oxid Met,2005;63:261 [4]Bridges D W,Baur J P,Baur G S,Fassell W M.J Elec- trochem Soc,1956;103:475 [5]Wallwork G R.,Smeltzer W W.Corros Sci,1969;9:561 [6]Mrowec S.Oxid Met,1973;6:178 [7]Garnaud G.Oxid Met,1977;11:127 [8]Hoar T P,Price L E.Trans Faraday Soc,1938;34:867 [9]Zhu R Z,He Y D,Qi H B.High-temperature Corro- sion and Resisting High-temperature Corrosion Materi- als.Shanghai:Shanghai Science and Technology Press, 1995:99 (朱日彰,何业东,齐慧滨.高温腐蚀及耐高温腐蚀材料.上海:上海科学技术出版社,1995:99) [10]Li T F.High Temperature Oxidation and Hot Corrosion of Metals.Beijing:Chemical Industry Press,2003:52 (李铁藩.金属高温氯化和热腐蚀.北京:化学工业出版社,2003:52) [11]Evans U R.The Corrosion and Oxidation of Metals.Lon- don:Edward Arnold Ltd,1968;696:701 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|