| 薄板坯连铸连轧工艺生产的Nb、Ti复合微合金化热轧带钢的强化机制 |
| 王瑞珍;章洪涛 |
| 钢铁研究总院结构材料研究所; 北京 100081 |
|
引用本文:
王瑞珍; 章洪涛 . 薄板坯连铸连轧工艺生产的Nb、Ti复合微合金化热轧带钢的强化机制[J]. 金属学报, 2007, 43(10): 1082-1090 .
[1]DeArdo A J,Garcia C I,Palmiere E J.ASM Handbook, Vol.4,Heat Treating,Materials Park,OH,ASM Interna- tional,1990:237 [2]Kang Y,Yu H,Wang K,Fu J,Liu D,Wang Z,Li L,Chen G.Proc Int Symp Thin Slab Casting Rolling,Guangzhou, China:The Chinese Society for Metals,2002:313 [3]Baker T N,Li Y,Wilson J A,Craven A J,Crowther D N. Mater Sci Technol,2004;20:720 [4]Wang R,Hua M,Zhang H,Carcia C I.HSLA Steels 2005, Sanya,China,The Chinese Scoiety for Metals,2005:292 [5]Thillou V.Basic Metal Processing Research Institute Re- port,University of Pittsburgh,PA,USA,1997 [6]Ma X.Phys Test Chem Anal.Part B:Chemical Analysis, 1985;21(4):215 (马翔.理化检验化学分册,1985;21(4):215) [7]Jia Y H,Lu C F,Liu Q B.Metall Anal,2004;24(Suppl): 463 (贾云海,卢翠芬,刘庆斌.冶金分析,2004;24(Suppl):463) [8]Honeycombe R W K,Smith G M.In:Gifkins R C ed., Int Conf ICSMA 6 Strength Met Alloy,Pergamon Press, 1982:407 [9]Garcia J E.Master Thesis,University of Pittsburgh,2002 [10]Jun H J,Kang K B,Park C G.Scr Mater,2003;49:1081 [11]Yong Q L,Ma M T,Wu B R.Microalloyed Steels—Physical and Mechanical Metallurgy.Beijing:China Ma- chine Press,1989:57 (雍岐龙,马鸣图,吴宝榕.微合金钢—物理和力学冶金.北京:机械工业出版社,1989:57) [12]Ashby M F.Strengthening Methods in Crystals.London: Applied Science Publishers Ltd,1971:137 [13]Gladman T,Dulieu D,Mcivor T D.Proc Int Conf Mi- croalloying'75,New York:Union Carbide Corporation, 1977:32 [14]Hong S G,Jun H J,Kang K B,Park C G.Scr Mater, 2003;48:1201 [15]Garcia C I,Ruiz-Aparicio A,Cho K,Ma Y,Graham C, Vazquez M,Ruiz-Aparicio L.Proc Int Syrup Thin Slab Casting Rolling,Guangzhou,China:The Chinese Society for Metals,2002:397 [16]Kothe A,Kunze J,Backmann G,Mickel C.Mater Sci Forum,1998;284-286:493 [17]Kneissl A C,Garcia C I,DeArdo A J.Proc Int Conf Processing,Microstructure and Properties Microalloyed Other Modern High Strength Low Alloy Steels,Warren- dale,PA:ISS,1991:145 [18]Kejian H,Baker T N.In:Baker T Ned.,Proc Conf Tita- nium Technol Microalloy Steel,London:The Inst Mater, 1997:115 [19]Craven A J,He K,Garvie L A J,Baker T N.Acta Mater, 2000;48:3857 [20]DeArdo A J,Marraccini R,Hua M J,Garcia C I.HSLA Steels 2005,Sanya,China,The Chinese Society for Met- als,2005:23 [21]Fernandez A I,Uranga P,Lopez B,Rodriguez-Ibabe J M. Mater Sci Eng,2003;A361:367 [22]Fernandez A I,Uranga P,Lopez B,Rodriguez-Ibabe J M. ISIJ Int,2000;40:893 [23]de Ardo A J.Conf Proc Niobium Science Technology.Or- lando,Florida,USA:Niobium.2001 Limited,2001:427 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|