| 焊接参数对搅拌摩擦焊接构件搅拌区材料融合的影响 |
| 张昭 张洪武 |
| 大连理工大学工程力学系 |
|
| EFFECT OF WELDING PARAMETERS ON MIXTURE OF MATERIALS IN NUGGET ZONE IN FRICTION STIR WELDS |
引用本文:
张昭; 张洪武 . 焊接参数对搅拌摩擦焊接构件搅拌区材料融合的影响[J]. 金属学报, 2007, 43(3): 321-326 .
[1]Mishra R S,Ma Z Y.Mater Sci Eng,2005;R50:1 [2]Liu H J,Chen Y C,Feng J C.Scr Mater,2006;55:231 [3]Feng J C,Chen Y C,Liu H J.Mater Sci Technol,2006; 22:86 [4]Zeng W M,Wu H L,Zhang J.Acta Metall Sin(Engl Lett), 2006;19:9 [5]Ma Z Y,Mishra R S,Mahoney M W.Acta Mater,2002; 50:4419 [6]Ma Z Y,Mishra R S.Scr Mater,2005;53:75 [7]Ma Z Y,Sharma S R,Mishra R S.Sct Mater,2006;54: 1623 [8]Xu S W,Deng X M,Reynolds A P,Seidel T U.Sci Technol Weld Joining,2001;6:191 [9]Deng X M,Xu S W.J Manuf Process,2004;6:125 [10]Fonda R W,Lambrakos S G.Sci Technol Weld Joining, 2002,7:177 [11]Schmidt H,Hattel J.Sci Technol Weld doining,2005;10: 176 [12]Khandkar M Z H,Khan J A,Reynolds A P,Sutton M A. J Mater Process Technol,2006;174:195 [13]Zhang H W,Zhang Z,Chen J T.Acta Metall Sin,2005; 41:853 (张洪武,张昭,陈金涛.金属学报,2005;41:853) [14]Zhang H W,Zhang Z,Chen J T.Mater Sci Eng,2005; A403:340 [15]Zhang z,Chen J T,Zhang H W.J Aeronaut Mater,2005; 25(6):33 (张昭,陈金涛,张洪武.航空材料学报,2005;25(6):33) [16]Zhang Z,Chen J T,Zhang H W.J Mater Eng,2006;(1): 19 (张昭,陈金涛,张洪武.材料工程,2006;(1):19) [17]Zhang H W,Zhang Z,Chen J T.Chin Mech Eng,2006; 17(7):719 (张洪武,张昭,陈金涛.中国机械工程,2006;17:719) [18]Zhang Z,Zhang H W.Ord Mater Sci Eng,2006;29(3): 61 (张昭,张洪武.兵器材料科学与工程,2006;29(3):61) [19]Zhang H W,Zhang Z,Chen J T.Trans Chin Weld Inst, 2005;26(9):13 (张洪武,张昭,陈金涛.焊接学报,2005;26(9):13) [20]Zhang Z,Zhang H W.Acta Metall Sin,2006;42:998 (张昭,张洪武.金属学报,2006;42:998) [21]Ponthot J P.J Mater Process Technol,1998,80-81:628 [22]Belytschko T,Liu W K,Moran B.Nonlinear Finite El- ??ements for Continua and Structures.New York:John Wiley & Sons Ltd,2000:131 [23]HKS Inc.ABAQUS Theory Manual,V6.4,Hibbt,Karls- son and Sorensen Inc.,2003 [24]Simo J C,Hughes T J R.Computational Inelasticity,New York:Springer,1998:153 [25]Potdar Y K,Zehnder A T.J Manuf Sci Eng,2003;125: 645 [26]Chen C M,Kovacevic R.Int J Mach Tools Manuf,2004; 44:1205 [27]Tang W,Guo X,McClure J C,Numes L E.J Mater Pro- cess Manuf Sci,1998;7:163 [28]Colegrove P,Painter M,Graham D,Miller T.Proc 2nd Int Syrup on Friction Stir Welding.Gothenburg:TWI Center,2000:162 [29]Fratini L,Buffa G.Int J Mach Tools Manuf,2005;45: 1188 [30]Marzoli L M,Strombeck A V,Dos Santos J F,Gambaro C,Volpone L M.Compos Sci Technol,2006;66:363Z |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|