| 氢渗透通过金属膜引起的塑性形变 |
| 侯民强 张武寿 |
| 中国科学院化学研究所 |
|
| PLASTIC DEFORMATION OF METALLIC MEMBRANE INDUCED BY HYDROGEN PERMEATION |
引用本文:
侯民强; 张武寿 . 氢渗透通过金属膜引起的塑性形变[J]. 金属学报, 2007, 43(3): 327-331 .
[1]Lewis A.The Palladium Hydrogen System.London:Aca- demic Press,1967:43 [2]Richter D,Hempelman R,Bowman R C Jr In:Schlap- bach L ed,Topics in Applied Physics.Berlin:Springer, 1992:67 [3]Wipf H.Topics in Applied Physics.Berlin:Springer, 1997:73 [4]Wang H Y,Fu Y B.Membrane Sci Technol,2002;22(6): 41 (王和义,傅依备.膜科学与技术,2002;22(6):41) [5]Hu Z L.Hydrogen Storage Materials,Bering:Chemical Industry Press.2002:52 (胡子龙,贮氢材料.北京:化学工业出版社,2005:52) [6]Li J C M.Metall Trans,1978;9 A:1353 [7]LarchéF C,Cahn J W.Acta Metall,1982;30:1835 [8]Lewis F A,Magennis J P,McKee S G,Seebuwufu P J M. Nature,1983;306:673 [9]Lewis F A,Baranowski B,Kandasamy K.J Less-Common Met,1987;134:L27 [10]Lewis F A,Tong X Q,Kandasamy K.Int J Hydrogen Energy,1993;18:481 [11]Tong X Q,Lewis F A.J Less-Common Met,1991;169: 157 [12]Tong X Q,Bucur R V.Kandasamy K,Lewis F A.Z Phys Chem(Neue Folge),1993;181:225 [13]Tong X Q,Lewis F A.Int J Hydrogen Energy,1995;20: 641 [14]Kandasamy K,Lewis F A,Magennis J P,McKee S G, Tong X Q.Z Phys Chem(Neue Folge),1991;171:213 [15]Kandasamy K,Tong X Q,Lewis F A.J Phys:Conden Mater,1992;4:L439 [16]Sakamoto Y,Tong X Q,Lewis F A.Scr Metall Mater, 1991;25:1629 [17]Baranowski B.J Less-Common Met,1989;154:329 [18]Dudek D,Baranowski B.Z Phys Chem(Neue Folge), ??1998;206:21 [19]Zhang W S,Zhang X W,Zhang Z L.Phys Rev,2000;62B: 8884 [20]Zhang W S,Zhang Z L,Zhang X W.J Alloys Compd, 2002;336:170 [21]Zhang W S,Zhang Z L,Zhang X W.J Alloys Compd, 2002;346:171 [22]Zhang W S,Hou M Q,Wang H Y,Fu Y B.Int J Hydrogen Energy,2004;29:1165 [23]Zhang W S,Hou M Q,Wang H Y,Fu Y B.Acta Mater, 2004;52:5805 [24]Hickman R G.J Less-Common Met,1969;19:369 [25]Baranowski B,Majchrzak S,Flanagan T B.J Phys F:Met Phys,1971;1:258 [26]Fukai Y.The Metal-Hydrogen System;Basic Bulk Prop- erties.Berlin:Springer,1993:Chapter 5 [27]Zhang W S,Zhang Z L,Zhang X W.j Electroanal Chem, 1999;474:130U |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|