| Mg-6Al-(Sr, Ca)合金的显微组织和蠕变性能 |
| 白 晶;孙扬善;薛 烽;薛 山;强 婧;陶卫健;刘海峰 |
| 东南大学材料科学与工程学院 |
|
| Microstructures and creep properties of Mg-6Al based magnesium alloys with strontium and calcium addition |
| 东南大学材料科学与工程系 |
引用本文:
白晶; 孙扬善; 薛烽; 薛山; 强婧; 陶卫健; 刘海峰 . Mg-6Al-(Sr, Ca)合金的显微组织和蠕变性能[J]. 金属学报, 2006, 42(12): 1267-1273 .
[1] Pekguleryuz M O. Mater Sci Forum, 2000; 350: 131 [2] Zeng R W, Ke W, Xu Y B, Han E H, Zhu Z Y. Acta Metall Sin, 2001; 37: 673 (曾荣伟,柯伟,徐永波,韩恩厚,朱自勇.金属学报,2001; 37:673) [3] Pekguleryuz M O, Baril E. Mater Trans, 2001; 42: 1258 [4] Pekguleryuz M, Labelle P, Argo D, Baril E. In: Kaplan H I ed, 2003 Magnesium Technology, Warrendale, PA: Minerals, Metals and Materials Society, 2003: 201 [5] Luo A A. Int Mater Rev, 2004; 49: 13 [6] Luo A A, Powell B R. In: Hryn J ed., Magnesium Technology 2001, Warrendale, PA: Minerals, Metals and Materials Society, 2001: 137 [7] Pekguleryuz M O, Kaya A A. Adv Eng Mater, 2003; 5: 866 [8] Blum W, Watzinger B, Zhang P. Adv Eng Mater, 2000; 2: 349 [9] Zhang P, Watzinger B, Blum W. Phys Status Solidi, 1999; 175A: 481 [10] Pekguleryuz M O, Baril E. In: Hryn J ed., Magnesium Technology 2001, Warrendale, PA: Minerals, Metals and Materials Society, 2001: 119 [11] Yuan G Y, Sun Y S, Zhang W M, Bao Y H. Ada Metall Sin (Engl Lett), 2000; 13: 867 [12] Min X G, Sun Y S, Du W W, Xue F. J Southeast Univ (Nat Sci), 2002; 32: 409 (闵学刚,孙扬善,杜温文,薛烽.东南大学学报(自然科学版),2002;32:409) [13] Regev M, Aghion E, Rosen A. Mater Sci Eng, 1997; A234- 236: 123 [14] Pekguleryuz M O, Baril E, Labelle P, Argo D. J Adv Mater, 2003; 35: 32 [15] Bradai D, Kadi H M. J Mater Sci, 1999; 34: 5331 [16] Xiao X L, Luo C P, Nie J F, Muddle B C. Acta Metall Sin, 2001; 37: 7 (肖晓玲,罗承萍,聂建锋,Muddle B C.金属学报,2001; 37:7) [17] Bai J, Sun Y S, Xun S, Xue F, Zhu T B. Mater Sci Eng, 2006; A419: 181 [18] Mordike B L, Lukac P. In: Lorimer G W ed., Proc 3rd Int Magnesium Conf, London: Institute of Materials, 1996: 419 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|