| 平行板型薄板坯连铸结晶器中钢液流动、凝固及溶质分布的三维耦合数值模拟 |
| 李中原;赵九洲 |
| 中科院金属研究所 |
|
| COUPLED NUMBERICAL SIMULATION ON SOLIDIFICATION AND SOLUTE TRANSPORT IN THIN SLAB CONTINUOUS CASTING PROCESS |
| 沈阳 |
引用本文:
李中原; 赵九洲 . 平行板型薄板坯连铸结晶器中钢液流动、凝固及溶质分布的三维耦合数值模拟[J]. 金属学报, 2006, 42(2): 211-217 .
[1] Tian N Y. Continuous Casting and Hot-roll of Thin Slab. Beijing: Metallurgical Industry Press, 1998: 3 (田乃媛,薄板坯连铸连轧.北京:冶金工业出版社.1998; 3) [2] Asai S, Szekely J. Ironmaking Steelmaking, 1975; 3: 205 [3] Thomas B G, Mika L J, Najjar F M. Metall Trans, 1990;21B: 387 [4] Huang X, Thomas B G, Najjar F M. Metall Trans, 1992;23B: 339 [5] Aboutalebi M R, Hasan M, Guthrie R I L. Metall Mater Trans, 1995; 26B: 731 [6] Flint P J. In: Spalding D B, ed., Proc 73rd Steelmaking Conf, Warrendale, PA: Iron and Steel Society, 1990: 481 [7] Zhu M Y, Sawada I. Ada Metall Sin, 1997; 33: 11 (朱苗勇,迟田郁夫.金属学报,1997; 33: 11) [8] Yang B J, Su J Y. Iron Steel, 1996; 31: 24 (杨秉俭,苏俊义.钢铁,1996; 31: 24) [9] Zhang H W, Wang E G, He J C. Ada Metall Sin, 2002;38: 99 (张红伟,王恩刚,赫冀成.金属学报,2002; 38: 99) [10] Yang H L, Zhao L G, Zhang X Z, Deng K W, Li W C,Gan Y. Metall Mater Trans, 1998; 29B: 1345 [11] Bao Y P, Zhu J Q, Jiang W, Zhang T, Tian N Y, Xu B M. J Univ Sd Technol Beijing, 2000; 24: 409 (包燕平,朱建强,蒋伟,张涛 ,田乃媛,徐宝美.北京科技大学学报,2000;24:409) [12] Yu H X, Zhang J M, Wang W J, Wang X H, Yang Z Y, Yang L X. J Univ Sd Technol Beijing, 2002; 26: 492 (于会香,张炯明,王万军,杨振亚,杨立新.北京科技大学学报,2002; 26:492) [13] Honeyands T, Herbertson J. Steel Res, 1995; 66(7): 287 [14] O'Connor T G, Dantzig J A. Metall Mater Trans, 1994;25B: 443 [15] Nam H, Park H S, Yoon J K. ISIJ Int, 2000; 40: 886 [16] Park H S, Nam H, Yoon J K. ISIJ Int, 2001; 41: 974 [17] Launder B E, Spalding D B. Comp Mater Appl Mech Eng,1974; 3: 269 [18] Carmon P C. Trans Ins Chem Eng, 1937; 15: 150 [19] Bennon W D, Incropera F P. Int J Heat Mass Trans, 1987;30: 2161 [20] Tao W Q. Numerical Heat Transfer. Xi'an: Xi'an Jiaotong University Press, 1988: 349 (陶文铨.数值传热学.西安:西安交通大学, 1988:349) [21] Patankar S V, translated by Zhang Z. Numberial Heat Transfer and Fluid Flow. Beijing: Science Press, 1984:131 (Patankar S V 著,张政译.传热与热体流动的数值计算.北京:科学出版社,1984:131) [22] Offerman C. Scand J Metall, 1981; 10: 25h |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|