| 阳极溶解促进α-Ti位错发射,运动导致SCC微裂纹形核 |
| 吕宏 王雪梅 |
| 北京科技大学材料物理系;北京 100083 |
|
引用本文:
吕宏; 王雪梅 . 阳极溶解促进α-Ti位错发射,运动导致SCC微裂纹形核[J]. 金属学报, 1999, 35(3): 232-238 .
[1] Chu W Y. Hydrogen Damage and Delayed Fracture. Beijing:Metallurgical Industrial Press, 1988: 361(褚武扬.氢损伤和滞后断裂.北京:冶金工业出版社,1988:361) [2] Sieradzki K, Newman R C. Philos Mag, 1985; 51A: 95 [3] Galvele J R. Corros Sci, 1987; 27: 1 [4] Jones D A. Metall Trans, 1985; 16A: 1133 [5] Magnin T Chieragatti R, Oltra R. Acta Metall Mated 1990;38: 1313 [6] Kaufman M J, Fink J I. Acta Metall, 1985; 36: 2213 [7] Flanagan W F, Bastias P, Lichter B D. Acta Metall Mater,1991; 39: 695 [8] Revie R W, Uhlig H H. Acta Metall, 1974; 22: 619 [9] Uhlig H H. i Eloctrochem Soc, 1976; 123: 1669 [10] Gu B, Chu W Y, Qiao L J, Hsiao C M. Corros Sci, 1994; 36:1437 [11] Gu B, Gao K W, Huang Y Z, Chu W Y. Sci Chin, 1966;26E: 481(谷飚,高克玮,黄一中,褚武扬.中国科学,1996; 26E:481) [12] Gu B, Zhang J W, Wan F R, Chu W Y. Scr Metall Mater,1995; 32: 637 [13] Nelson J C, Oriani R A. Corros Sci, 1993; 34: 307 [14] Lu H, Gao K W, Chu W Y. Scr Mater, 1997; 37: 1387 [15] Ohr S M. Mater Sci Eng, 1983: 59: 1 [16] Zhu T, Yang W, Guo T. Acta Mater, 1996; 44: 3049 [17] Zhang T C, Chu W Y. Acta Metall Sin, 1997; 33: 309)(张天成,褚武扬.金属学报,1997;33:309) [18] Evans H E. Int Mater Rev, 1995; 40: 1 [19] American Society for Metals. ASM Metals Reference Book.Metals Park, Ohio: ASM, 1983: 301 [20] Lian K, Meletis E I. Corros Sci, 1996; 52: 3476 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|