| Ni-Fe-Cr-Ti及Co-Ni-Fe-Cr-Ti(Si, B)系高温钎料对Si3N4陶瓷的润湿与界面连接 |
| 熊华平 程耀永 |
| 北京航空材料研究院焊接与锻压工艺研究院; 北京 100095 |
|
引用本文:
熊华平; 程耀永 . Ni-Fe-Cr-Ti及Co-Ni-Fe-Cr-Ti(Si, B)系高温钎料对Si3N4陶瓷的润湿与界面连接[J]. 金属学报, 2000, 36(12): 1269-1274 .
[1] Naka M, Kubo M. J Mater Sci, 1987; 22: 4417 [2] Naka M, Kubo M. Trans JWRI, 1990; 19(2): 21 [3] Naka M, Kubo M. Trans JWRI, 1987; 16(1): 83 [4] Okamura H. Welding Int, 1993; 7: 236 [5] Kang S, Kim H J. Welding J, 1995; 74: 289s [6] Tillmann W, Lugscheider E, Schlimbach K, Manter C, Indacochea J E. Welding J, 1998; 77: 103s [7] Chen J H, Wang G Z. J Mater Sci Lett, 1993; 12: 87 [8] Lu S P, Guo Y, Chen L S. In: Wang S Y, Wang L S eds.,Proc 8th Annual Symposium on Welding of China, Vol.1,Beijing: Machinery Industry Press, 1997; 274(陆善平,郭义,陈亮山.见:王守业,王麟书主编,第八次全国焊接会议论文集,第1卷,北京:机械工业出版社,1997:274) [9] Lu S P, Dong X Z, Wu Q, Guo Y. Chin J Mater Res,1998; 12: 295(陆善平,董秀中,吴庆,郭义.材料研究学报,1998;12:295) [10] Wan C G, Kritsalis P. J Mater Sci Technol, 1994; 10: 466 [11] Feng J C, Qian Y Y. In: Wang S Y, Wang L S eds., Proc8th Annual Symposium on Welding of China, Vol.I, Beijing: Machinery Industry Press, 1997; 321(冯吉才,钱乙余.见:王守业,王麟书主编,第八次全国焊接会议论文集,第1卷,北京:机械工业出版社,1997:321) [12] Xiong H P, Wan C G, Zhou Z F. Metall Mater Trans,1998; 29A: 2591 [13] Liu C X. In: New Advances in Welding and AlliedProccesses-Proc Int Conf, 8-10 May 1991, Beijing, Sponsored by the Welding Institution of the Chinese Mechanical Engineering Society (WI CMES), and Deutscher Verband fur Schweisstechnik EV (DVS), International Academic Publishers, 1991: 345 [14] Klomp J T, Nicholas M G. Joining Ceramics. London:Champman & Hall, 1990: 113 [15] Miedema A R, Boer F R, Boom R, Dorleijn J W F. CALPHAD, 1977; 1: 353f |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|