| 考虑铸型阻力的铸件应力数值模拟 |
| 孙琨 朱东波 |
| 西安理工大学机械工程学院;西安 710049 |
|
引用本文:
孙琨; 朱东波 . 考虑铸型阻力的铸件应力数值模拟[J]. 金属学报, 2000, 36(12): 1258-1262 .
[1] Yang B J, Dantzig J A. Chin J Xi'an Jiaotong Univ, 1992;(8): 37(杨秉俭, Dantzing J A. 西安交通大学学报, 1992; (8): 37) [2] Chen Y, Bai X F, Zhu R M, Liu B C. Chin J Foundry,1997; (3): 1(陈瑶,白雪峰,朱日明,柳百成.铸造,1997;(3):1) [3] Deng K, Mao S G, Sun H C. Chin J Foundry Technol,1993; (2): 3(邓康,毛生根,孙焕纯.铸造技术,1993;(2:3) [4] Zheng X S, Yao S, Jin J Z. Chin J Dalian Univ Technol,1996; 11: 687(郑贤淑,姚山,金俊泽.大连理工大学学报,1996; 11:687) [5] Purvis A L, Pehlke R D. AFS Trans, 1992; 150: 593 [6] Lou Y, Yang J S, Wu P L. Chin J Foundry, 1997; (8): 7(楼易,杨际胜,吴培良.铸造,1997;(8):7) [7] Kang J W, Xiong S M, Liu B C. Chin J Foundry, 1999;(1): 23(康进武,熊守美,柳百成.铸造,1999;(1):23) [8] Jeffery W W, Jonathan A D. Metall Trans, 1990; 21A:489 [9] Zhang Y. Foundry-Technics CAD and Application. Beijing: Machinery Industruak Press, 1994:140(张毅.铸造工艺CAD及其应用.北京:机械工业出版社,1994:140) [10] Jiang Y Q, Mu X Y. Foundation of Plastic Mechanics.Beijing: Machinery Industrial Press, 1981: 20(蒋咏秋,穆霞英.塑性力学基础,北京:机械工业出版社,1981:20){ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|