| 铸铁件凝固过程中自然对流引起的宏观偏析模拟 |
| 杜强 李殿中 |
| 中国科学院金属研究所;沈阳 110015 |
|
引用本文:
杜强; 李殿中 . 铸铁件凝固过程中自然对流引起的宏观偏析模拟[J]. 金属学报, 2000, 36(11): 1197-1200 .
[1] Flemings M C, Mehrabian R, Nereo G G. Trans AIME,1968; 242: 41 [2] Bennon W D, Incropera F P. Int J Heat Mass Transfer,1987; 30: 2161 [3] Ni J, Beckermann C. Metall Trans, 1991; B22: 349 [4] Rappaz M. Int Mater Rev 1989; 34(3): 33 [5] Felicelli S D, Poirier D R, Heinrich J C. Metall MaterTrans, 1998; B29: 847 [6] Reddy A V, Beckermann C. Metall Mater Trans, 1997;B28: 479 [7] Gu J P, Beckermann C. Metall Mater Trans, 1999; A30:1357 [8] Moore B, Shah C. Int Mater Rev, 1983; 28: 345. [9] Schneider M C, Beckermann C. Int J Heat Mass Transfer,1995: 298 [10] Patankar S V. Numerical Heat Transfer and Fluid Flow.New York: McGraw-Hill, 1980: 131 [11] Clyne T W, Kurz W. Metall Trans, 1981; A12: 965 |
|