| 熔体过热历史对Ni基高温合金定向凝固界面形态的影响 |
| 陈光 俞建威 谢发勤 傅恒志 |
| 南京理工大学材料科学与工程系;南京210094 |
|
引用本文:
陈光; 俞建威; 谢发勤; 傅恒志 . 熔体过热历史对Ni基高温合金定向凝固界面形态的影响[J]. 金属学报, 2001, 37(5): 488-492 .
[1] Li P J, Gui M C, Jia J, Li Q C, Ri C Foundry, 1995; (9):15 (李培杰,桂满昌,贾钧,李庆春,里豪森.铸造,1995;(9): [2] Zhang L, Bian X F, Ma J J. Foundry, 1995; (10): 7 (张林,边秀房,马家骥.铸造,1995;(10):7) [3] Guan S K. Ph D Thesis, University of Science and Technology Beijing, 1995 (关绍康.博士学位论文,北京科技大学,1995) [4] Jian Z Y. Ph D Thesis, Northwestern Polytechnical University, 1995 (坚增运.博士学位论文,西北工业大学,1995) [5] Chen G, Cai Y W, Li J G, Fu H Z. J Hebei Univ SciTechnol, 1998; 19(1): 6 (陈光,蔡英文,李建国,傅恒志.河北科技大学学报,1998; [6]1992; (7): 21 [7] Gui Z L. Aviation Production Eng, 1995; (4): 12 (桂忠楼.航空制造工程,1995;4:12) [8] Tiller W A, Jackson K A, Rutter J W, Chaluers, B. ActaMetall, 1953; 1: 428 [9] Mullins W W, Sekerka R F. J Appl Phys, 1964; 35: 444 [10] Wollkind D J, Segel L A. Phil Trans Roy Soc, 1970; 268:351 [11] Li J G, Mao X M, Fu H Z. Acta Metall Sin, 1990; 26:A309 (李建国,毛协民,傅恒志.金属学报,1990;26:A309) [12] Gill S C, Kurz W. Mater Sci Eng, 1993; A173: 335 [13] Chen G, Yu J W, Fu H Z. J Mater Sci Lett, 1999; 18:1571 [14] Chen G, Yu J W, Sun Y C, Fu H Z. Chin J Mater Res,1999; 13: 497 (陈光,俞建威,孙彦臣,傅恒志.材料研究学报,1999;13:497) [15] Li R S. Non-Equilibrium Thermodynamics and Dissipation Structure. Beijing: Tsinghua Univ Press, 1986: 55 (李如生.非平衡态热力学和耗散结构.北京:清华大学出版社,1986:55) [16] Mao X M, Fu H Z, Zhou Y H. Metall Sci Tech, 1986; 5(3):1 (毛协民,傅恒志,周尧和.金属科学与工艺,1986;5(3):1) [17] Chen C L, Lu F Y. Acta Metall Sin, 1997; 33: 455 (陈长乐,陆福一.金属学报,1997;33:455) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|