| 通过基体合金化制备界面相容的Al2O3p/Al颗粒增强铝基复合材料 |
| 李斗星 周朝霞 樊中云 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室;沈阳110016 |
|
引用本文:
李斗星; 周朝霞; 樊中云 . 通过基体合金化制备界面相容的Al2O3p/Al颗粒增强铝基复合材料[J]. 金属学报, 2002, 38(6): 602-608 .
[1] Yung T. Philos Trans Roy Soc, 1805: 95 : 65 [2] Polmear I J. Light Alloys: Metallurgy of the Light Metals.London: Edward Arnold LTD, 1981; 16 [3] Beer S Z. Liquid Metals: Chemistry and Physics.NewYork: Dekker, 1972; 127 [4] Moore J J. Chemical Metallurgy. London-Boston: But-terworths, 1981; 87 [5] Zhou Z, Peng H X, Fan Z, Li D X. Mater Sci Tech, 2000;16: 908 [6] Wu G H, Ma S L, Zhao Y C, Yang D Z.Chin J MaterRes, 1998; 12: 307 (武高辉,马森林,赵永春,杨德庄.材料研究学报,1998;12:307) [7] Redsten A M, Klier E M, Brown A M, Dunand D C. MaterSci Eng A, 1995; A201: 88 [8]Zhou Z, Fan Z, Peng H X, Li D X. J Microscopy, 2001;201:144- |
|