| Zn-2%Cu包晶合金定向凝固的微观组织 |
| 王猛 林鑫 苏云鹏 沈淑娟 黄卫东 |
| 西北工业大学凝固技术国家重点实验室;西安710072 |
|
引用本文:
王猛; 林鑫; 苏云鹏; 沈淑娟; 黄卫东 . Zn-2%Cu包晶合金定向凝固的微观组织[J]. 金属学报, 2002, 38(4): 337-341 .
[1] Kerr H W, Kurz W. Int Mater Rev, 1996; 4: 41 [2] Chalmers B. Physical Metallurgy. New York: John Wiley& Sons, 1959: 271 [3] Livingston J D. Mater Sci Eng, 1971; 7: 61 [4] Flemings M C. Solidification Processing. New York:McGraw-Hill, 1974: 177 [5] Boetingger W J. Metall Trans, 1974; 5A: 2023 [6] Lee J H, Verhoeven J D. J Cryst Growth, 1994; 144: 353 [7] Busse P, Meissen F. Scr Mater, 1997; 36: 653 [8] Vandyoussefi M, Kerr H W, Kurz W. Acta Mater, 2000;48: 2297 [9] Xu W, Ma D, Feng Y P, Li Y. Scr Mater, 2001; 44. 631 [10] Ma D, Li Y, Ng S C, Jones H. Acta Mater, 2000; 48: 419 [11] Perepezko J H, Boetingger W J. Mater Res Soc SympProc, 1983; 19: 223 |
|