Please wait a minute...
金属学报  2002, Vol. 38 Issue (11): 1141-1148     
  论文 本期目录 | 过刊浏览 |
TiAl基合金新材料研究及精密成形
陈玉勇  孔凡涛
哈尔滨工业大学材料科学与工程学院金属精密热加工国家重点实验室;哈尔滨150001
引用本文:

陈玉勇; 孔凡涛 . TiAl基合金新材料研究及精密成形[J]. 金属学报, 2002, 38(11): 1141-1148 .

全文: PDF(328 KB)  
摘要: TiAl基合金以其低密度、高强度以及良好的抗氧化性等特点得到广泛的研究.着重介绍了TiAl基合金在显微组织控制、组织-性能关系、合金化、熔炼技术、精密成形等方面的发展状况.
关键词 : TiAl基合金,  显微组织,  性能    
Key words:
收稿日期: 2002-04-17     
ZTFLH:  TG146.2  
[1] Kim Y W, Dimiduk D M. JOM, 1991; 43(8): 40
[2] Kim Y W. JOM, 1994; 7: 30
[3] Kim Y W. Trans Nonferrous Met Soc China, 1999; 9(Suppl.l): 298
[4] Edward A Loria. Intermetallics, 2000; 8: 1339
[5] Kumpfert J, Kim Y W, Dimiduk D M. Mater Sci Eug,1995; A192/193: 465
[6] Dimiduk D M, Mcquay P A, Kim Y W. In: Ushkov G ed, Titanium'99: Science and Technology, St Petersburg, CRISM Prometey, Russia, 1999: 259 [7] Hu D. Intermetallics, 2001; 9: 1037 [8] Ramanujan R V. Int Mater Rev, 2000; 45(6): 217 [9] Zhang D, Arzt E, Clemens H. Intermetallics, 1999; 7: 1081 [10] Yang J, Wang J N, Wang Y, Xia Q F, Zhang B. Intermetallics, 2001; 9: 369
[11] Yun J H, Oh M H, Nam S W, Wee D M, Inui H, Yam-aguchi M. Mater Sci Eng, 1997; A239-240: 702
[12] Kong F T, Dong M H, Chen Y Y. J Chin Rare Earth Soc, 2002; 1: 72(孔凡涛,董孟环,陈玉勇.中国稀土学报,2002;1:72)
[13] Atsumi O. The Solidification of Metals. Tokyo: ChijinShokan Co. Ltd, 1976: 95
[14] Tang J C, Huang B Y, Zhou K C, Liu W S, He Y H, LiuY. Mater Res Bull, 2001; 36: 1737
[15] Park H S, Nam S W, Kim N J, Hwang S K. Scr Mater,1999; 41: 1197
[16] Maziasz P J, Ramanujan R V, Liu C T, Wright J L. In-termetallics, 1997; 5: 83
[17] Kong F T, Chen Z Y, Tian J, Chen Y Y. Rare Met MaterEng, 2002; to be accepted(孔凡涛,陈子勇,田 竞;陈玉勇.稀有金属材料与工程,2002;待发表)
[18] Liu C T, Maziasz P J. Intermetallics, 1998; 6: 653
[19] Chen Y Y, Kong F T. Trans Nonferrous Met Soc China,2002; to be accepted
[20] Wang J N, Xie K. Intermetallics, 2000; 8: 545
[21] Nazmy M, Staubli M. Scr Metall Mater, 1994; 31: 829
[22] Beddoes J, Wallace W, Zhao L. Int Mater Rev, 1995; 40:197
[23] Blavette D, Duval P, Letellier L, Guttmann M. ActaMater, 1996; 44: 4995
[24] Perdrix F, Trichet M F, Bonnentien J L, Cornet M, BigotJ. Intermetallics, 2001; 9: 147
[25] Nam C Y, Wee D M, Wang P, Kumar K S. Intermetallics,2002; 10: 113
[26] Zhang L T, Qiu G H, Wu J S. Scr Metall Mater, 1995;32: 1683
[27] Sun F S, Kim S, Cao C X, Lee Y T, Yan M G. Scr Mater,2001; 45: 383
[28] Akio H, Mitsuo H, Kojiro F K. Mater Sci Eng, 1997;A239-240: 46
[29] Yin W M, Lupine V, Battezzati L. Mater Sci Eng, 1997;A239-240: 713
[30] Qin G W, Wang J J, Hao S M. Intermetallics, 1999; 7: 1
[31] Chen G L, Zhang L C, Zhang W J. Intermetallics, 1999;7: 1211
[32] Kumpfert J, Kim Y W, Dimiduk D M. Mater Sci Eng,1995; A192-193: 465
[33] Kim Y W. Intermetallics, 1998; 6: 623
[34] Zhe J, George T G, Kim Y W. Mater Sci Eng, 1997; A239-240: 729
[35] Leholm R, Clemens H, Kestler H, Bartolotta P. In:Ushkov G ed, Titanium'99: Science and Technology, StPetersburg, CRISM Prometey, Russia, 1999: 269
[36] Inkson B J, Clemens H, Marien J. Scr Mater, 1998; 38:1377
[37] Bartels A, Schillinger W. Intermetallics, 2001; 9: 883
[38] Bartels A, Hartig Ch , Willems St, Uhlenhut H. Mater SciEng, 1997; A239-240: 14
[39] Gouma P I, Davey S J, Loretto M H. Mater Sci Eng, 1998;A241: 151
[40] Du X W, Wang J N, Zhu J. Intermetallics, 2001; 9: 745
[41] Beddoes J, Zhao L, Au P, Wallace W. Mater Sci Eng,1995; A192/193: 324
[42] Noda T. Intermetallics, 1998; 6: 709
[43] Eylon D, Keller M M, Jones P E. Intermetallics, 1998; 6:703
[44] Kim M C, Oh M H, Lee J H, Inui H, Yamaguchi M, WeeD M. Mater Sci Eng, 1997; A239-240: 570
[1] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强. 镍基高温合金表面冲击强化机制及应用研究进展[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[6] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[7] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[8] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[9] 刘伟, 陈婉琦, 马梦晗, 李恺伦. 聚变堆用W在等离子体作用下的辐照损伤行为研究进展[J]. 金属学报, 2023, 59(8): 986-1000.
[10] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[11] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[12] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[13] 孙蓉蓉, 姚美意, 王皓瑜, 张文怀, 胡丽娟, 仇云龙, 林晓冬, 谢耀平, 杨健, 董建新, 成国光. Fe22Cr5Al3Mo-xY合金在模拟LOCA下的高温蒸汽氧化行为[J]. 金属学报, 2023, 59(7): 915-925.
[14] 张德印, 郝旭, 贾宝瑞, 吴昊阳, 秦明礼, 曲选辉. Y2O3 含量对燃烧合成Fe-Y2O3 纳米复合粉末性能的影响[J]. 金属学报, 2023, 59(6): 757-766.
[15] 郭福, 杜逸晖, 籍晓亮, 王乙舒. 微电子互连用锡基合金及复合钎料热-机械可靠性研究进展[J]. 金属学报, 2023, 59(6): 744-756.