| 液-固相轧制法生产Al-8Sn-2.5Si-2Pd-0.8Cu-0.2Cr/钢复合轴瓦带的组织与性能 |
| 许光明 崔建忠 |
| 东北大学材料电磁过程研究教育部重点实验室 110004 |
|
引用本文:
许光明; 崔建忠 . 液-固相轧制法生产Al-8Sn-2.5Si-2Pd-0.8Cu-0.2Cr/钢复合轴瓦带的组织与性能[J]. 金属学报, 2003, 39(7): 725-728 .
[1] Whitney W. In: SAE Technical Paper Sevies, Detroit Michigan: The Engineering Society for Advancing Mobility Land Sea Air and Space International Congress and Exposition, 1995: 950953 [2] Dai L F, Zhang C H, Dai K L, Xie G C. Min Metall Eng, 2000; 20: 67(戴兰芳,张春华,代孔林,谢刚朝.矿冶工程,2000;20:67) [3] Jin Z M, He J C, Di H S. Chin J Comput Phys, 1999; 16: 409(金珠梅,赫冀成,邸宏双.计算物理,1999;16:409) [4] Zhu Q, Pan D W, Zhang W Q. Steel Rolling, 1989; (4) : 19(朱泉,潘大炜,张文奇.轧钢,1989;(4) :19) [5] Jiang Y Q, Hou F J, Sun Y J. Mater Technol Automotive, 1999; (3) : 16(蒋玉琴,侯福建,孙亚军.汽车材料和工艺,1999;(3) :16) [6] Yuan G C, Li Z J, Lou Y X, Zhang X M. Chin J Nonferrous Met, 1997; 7: 110(袁鸽成,黎祚坚,娄燕雄,张新明.中国有色金属学报,1997;7:110)2 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|