| 二次硬化合金钢中多组元强化相M2C碳化物的粗化动力学研究 |
| 胡正飞; 吴杏芳; 王春旭 |
| 北京科技大学材料物理系; 北京 100083 |
|
引用本文:
胡正飞; 吴杏芳; 王春旭 . 二次硬化合金钢中多组元强化相M2C碳化物的粗化动力学研究[J]. 金属学报, 2003, 39(6): 585-591 .
[1] Kuo K. J Iron Steel Ins, 1953; 173: 223 [2] Hu Z F, Wu X F, Wang C X. Acta Metall Sin, 2001; 37: 381(胡正飞,吴杏芳,王春旭.金属学报,2001;37:381) [3] Allen A J, Gavillet D, Weertman J R. Acta Metall Mater, 1993; 41: 1969 [4] Montgomery J S, Olson G B. In: Olson G B ed, Proc 34th Sagamore Army Materials Researeh Conf, US Army Materials Technology Laboratory, Watertown, MA, 1990: 147 [5] Hu Z F, Wu X F, Wang C X. J Mater Eng Perf, 2001; 10: 493 [6] Bhattacharyya S K, Russell K C. Metall Trans, 1972; 3: 2195 [7] Bjorklund S, Donaghey L F, Hillert M. Acta Metall, 1972; 20: 867 [8] Lee H M, Allen S M, Gruicic M. Metall Trans A, 1991; 22A: 2863 [9] Speich G R, Dabkowski D S, Porter L F. Metall Trans, 1973; 4: 303 [10] Ghosh G, Campbell C E, Olson G B. Metall Mater Trans A, 1999; 30A: 501 [11] Hu Z F, Wu X F, Wang C X. In: Zhao X F ed, Proc of 9th Inter Conf BCEIA, Part A, Peking Univ Press, Beijing, 2001: 105 [12] Grujicic M, Olson G B. CALPHAD, 1988; 12: 405 [13] Grujicic M. Mater Sci Eng, 1989; A117: 215 [14] Lifshitz I M, Slyoov V V. J Phys Chem Solids, 1961; 19: 35 [15] Wagner C. Z Elektrochem, 1961; 65: 581 [16] Vengreovitch R D. Acta Metall, 1982; 30: 1079 [17] Mukjerhee T, Saumpf W E, Swllars C M, Tegart W J. J Iron Steel Inst, 1969; 207: 621 [18] Cahn J W. Acta Metall, 1980; 28: 1333 [19] Johnson C A. Surf Sci, 1965; 6: 335 [20] Ham F S. J Phys Chem Solids, 1959; 6: 335 [21] Johnson W C, Voorhees P W. Metall Trans A, 1987; 18A: 1213 [22] Bhattacharyya S K, Russell K C. Metall Trans A, 1976; 7A: 453 [23] Fujita N, Bhadeshia H K D H. Mater Sci Tech, 1999; 15: 627 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|