| 硼含量对镍基合金GH4049晶界析出相和高温性能的影响 |
| 陈国胜;金 鑫;周奠华;王世普;谢 伟;王林涛 |
| 宝钢集团特钢技术中心; 上海 200940 |
|
| Effects of Boron Content on Boundaries Precipitates in Ni Base Alloy GH4049 and Its High Temperature Properties |
| CHEN Guosheng; JIN Xin; ZHOU Dianhua; WANG Shipu; XIE Wei; WANG Lintao |
| Special Steel Technical Center; Baosteel Group; Shanghai 200940 |
引用本文:
陈国胜; 金鑫; 周奠华; 王世普; 谢伟; 王林涛 . 硼含量对镍基合金GH4049晶界析出相和高温性能的影响[J]. 金属学报, 2005, 41(6): 622-626 .
,
,
,
,
,
.
Effects of Boron Content on Boundaries Precipitates in Ni Base Alloy GH4049 and Its High Temperature Properties[J]. Acta Metall Sin, 2005, 41(6): 622-626 .
[1]Franzoni U,Marchetti F,Sturlese S.Scr Metall,1985;19:511 [2]Cao W D,Kennedy R L.In:Kissinger R D,Deye D.J.Anton D L,Cetel A D,Nathal M V,Pollock T M,Wood-ford D A,eds.,Superalloys 1996,Warrendale,PA:TMS AIME,1996:589 [3]Kennedy R L,Cao W D,Thomas W M.Adv Mater Process,1996;149(3):33 [4]Gorokhov V P,Kolachev B A,Parfenova O A,Novikova M B.Metall Heat Treat Met,2003;(4):22 [5]Letellier L,Chambreland S,Duval P.Appi Surf Sci,1993;67:305 [6]Letellier L,Guttmann M,Blavette D.Philos Mag Lett,1994;70:189 [7]Horton J A,McKamey C G,Miller M K,Cao W D,Kennedy R L.In:Loria E A,ed.,Superalloys 718,625,706 and Various Derivatives,Warrendale,PA:TMS AIME,1997:401 [8]Lemarchand D,Cadel E,Chambreland S,Blavette D.Philos Mag,2002;82A:1651 [9]Miller M K,Anderson I M,Pike L M,Klarstrom D L. Mater Sci Eng,2002;A327:89 [10]Li Y Q,Liu J Y.High Temp Technol,1990;8:278 [11]Li Y Q,Xu B W,Li Q K.Mater High Temp,1992;10:219 [12]Li Y Q,Chen G S,Zhang J F,Liu J Y.Prog Nat Sci, 2000;10:331 [13]Liu L R,Jin T,Zhao N R,Sun X F,Guan H R,Hu Z Q.Mater Sci Bng,2003;A361:191H |
|