| 微电化学技术研究双相不锈钢优选腐蚀行为 |
| 付燕;林昌健;蔡文达 |
| 厦门大学化学系固体表面物理化学国家重点实验室; 厦门 361005 |
|
| A study of the selective dissolution behavior of duplex stainless steel by micro-electrochemical technique |
| FU Yan; LIN Changjian; TSAI Wen-Ta |
| State Key Laboratory for Physical Chemistry of Solid Surfaces; Department of Chemistry;Xiamen University; Xiamen |
引用本文:
付燕; 林昌健; 蔡文达 . 微电化学技术研究双相不锈钢优选腐蚀行为[J]. 金属学报, 2005, 41(3): 302-306 .
,
,
.
A study of the selective dissolution behavior of duplex stainless steel by micro-electrochemical technique[J]. Acta Metall Sin, 2005, 41(3): 302-306 .
[1] Wu J. Corros Prot Oil Chem Eng, 1996; 13(1): 6 (吴玖.石油化工腐蚀与防护, 1996;13(1):6) [2] Qin Z R, Li L S, Liu D J. Dev Appl Mater, 1995; 10(5): 8 (秦紫瑞,李隆盛,刘德经.材料开发与应用,1995;10(5):8) [3] Wu J et al. Duplex Stainless Steel. Beijing: Metallurgical Industry Press, 1999: 459 (吴玖等.双相不锈钢.北京:冶金工业出版社,1999:459) [4] Xuan Z N, Chen K F. Chin Pulp Paper Ind, 2002; 23(9): 43 (宣征南,陈克复.中华纸业, 2002;23(9):43) [5] Sridhar N, Kolts J. Corrosion, 1987; 43: 648 [6] Symniotis E. Corrosion, 1990; 46: 2 [7] Yau Y H, Steicher M A. Corrosion, 1987; 43: 366 [8] Aldykiewicz A J, Isaacs H S. Corros Sci, 1998; 40: 1627 [9] Tsai W T, Tsai K M, Lin C J, Fu Y. Electrochem, 2003; 9: 170 [10] Femenia M, Pan J, Leygraf C. Corros Sci, 2001; 43: 1939 [11] Femenia M, Canalias C, Pan J, Leygraf C. J Electrochem Soc, 2003; 150: B274 [12] Pan J, Femenia M, Canalias C. Electrochem Soc Proc, 1999; 99(28): 131 [13] Dias A, Andrade M S. Appl Surf Sci, 2000; 161: 109 [14] Park J O, Suter T, Bohni H. Corrosion, 2003; 59: 59 [15] Suter T, Bohni H. Electrochim Acta, 2001; 47 (1-2): 191 [16] Webb E G, Alkire R C. J Electrochem Soc, 2002; 149: B272 [17] Perren R A, Suter T A, Uggowitzer P J, Weber L, Mag- dowski R, Bohni H, Speidel M O. Corros Sci, 2001; 43: 707 [18] Perren R A, Suter T A, Uggowitzer P J. Corros Sci, 2001; 43: 727 [19] Yau Y H, Steicher M A. Corrosion, 1987; 43: 366 [20] El-Dahshan M E, El Din A M S, Haggag H H. Desalination, 2002; 142: 161 [21] Davis G O, Kolts J, Sridhar N. Corrosion, 1986; 42: 329 |
|