镁合金与铝合金压铸过程中型腔内压力的变化特性 |
刘文辉 刘艳改 熊守美 柳百成 Y. Matsumoto; M. Murakami |
清华大学机械工程系; 北京 100084 |
|
Comparative Study of the Cavity Pressure of Magnesium Alloy and Aluminium Alloy During Die Casting Process |
LIU Wenhui; LIU Yangai; XONG Shoumei; LIU Baicheng;Y. Matsumoto; M. Murakami |
Mechanical Engineering Department; Tsinghua University; Beijing 100084 |
引用本文:
刘文辉; 刘艳改; 熊守美; 柳百成; Y.Matsumoto; M.Murakami . 镁合金与铝合金压铸过程中型腔内压力的变化特性[J]. 金属学报, 2005, 41(1): 103-.
,
,
,
,
,
.
Comparative Study of the Cavity Pressure of Magnesium Alloy and Aluminium Alloy During Die Casting Process[J]. Acta Metall Sin, 2005, 41(1): 103-.
[1] Tanikawa D, Asai K, Nomura H, Kato E. 2002 Japan Die Casting Congress, 2002: 145 [2] Kubota S, Fujimaki D, Katoh T. 2002 Japan Die Casting Congress, 2002: 187 [3] Tong K S, Hu B H, Niu X P. J Mater Proc Technol, 2002; 127: 238 [4] Lin B N. Foundry Rheology. Harbin: Press of Harbin In- stitute of Technology, 1991: 108 (林柏年.铸造流变学.哈尔滨:哈尔滨工业大学出版社.1991: 108) . [5] Li D F, Wang Z D. Nonferrous Met, 1997; (5): 4 (李德富,王志东.有色金属, 1997;(5):4) [6] Cheng J, Dang J Z, Cheng M, Zhao J P. J North Chin Inst Technol, 1995; (1): 9 (程军,党惊知,程眉,赵建平.华北工学院学报,1995; (1):9) [7] Wang B D, Liu Y, Li D F, Wang B X, Wang Z T. Met Forming Technol, 2003; (2): 40 (王炳德,刘莹,李德富,王本贤,王忠堂.金属成型工艺, 2003;(2):40)c |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|