| Zr基块状非晶的氢损伤与氢致滞后断裂 |
| 单广斌 王勇围 李金许 高克玮 宿彦京 乔利杰 惠希东 褚武扬 |
| 中国科学院金属研究所; 沈阳110016 |
|
| Hydrogen Damage and Delayed Fracture in Zr Base Bulk Metallic Glass |
| SHAN Guangbin; WANG Yongwei; LI Jinxu;GAO Kewei; SU Yanjing; QIAO Lijie;HUI Xidong;CHU Wuyang |
| Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
单广斌; 王勇围; 李金许; 高克玮; 宿彦京; 乔利杰; 惠希东; 褚武扬 . Zr基块状非晶的氢损伤与氢致滞后断裂[J]. 金属学报, 2005, 41(1): 99-.
,
,
,
,
,
,
,
.
Hydrogen Damage and Delayed Fracture in Zr Base Bulk Metallic Glass[J]. Acta Metall Sin, 2005, 41(1): 99-.
[1] Viswanadham R K, Green J A S, Montague W G. ScrMetall, 1976; 10: 229 [2] Kawashina A, Hashimoto K. Scr Metall, 1980; 14: 41 [3] Ashock S, Stoloff N S, Glicksman M E, Slavin T. Scr Met-all, 1981; 15: 331 [4] Tong H S, Macur J E. Corrosion, 1982; 38: 464 [5] Schroeder H W, Koster U. J Non-Cryst Solids, 1983; 56:213 [6] Namboodhiri T K, Ramesh T A, Singh G, Seghal S. MaterSci Eng, 1983; 61: 23 [7] Flis J, Ashok S, Stoloff N S , Duguette D S. Acta Metall,1987; 56: 2071 [8] Lin J J, Perng T P. J Mater Sci Lett, 1991; 10: 1443 [9] Lin J J, Perng T P. Metall Mater Trans, 1995; 26A: 197 [10] Elaiz N, Eliezer D. Adv Perform Mater, 1999; 6: 5 [11] Duh D, Dauskardt R H. Scr Mater, 2000; 42: 233 [12] Duh D, Asoka-kumar P, Dauskardt R H. Acta Mater,2002; 50: 537 [13] Guo J X, Li J X, Qiao L J, Gao K W, Chu W Y. CorrosSci, 2003; 45: 735 [14] Chu W Y, Gao K W, Huang C H, Wang Y B, Qiao L J.Corrosion, 2000; 56: 1046 [15] Pan C, Su Y J, Chu W Y, Li Z B, Liang D T, Qiao L J.Corros Sci, 2002; 44: 1983 [16] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environmental Fracture. Beijing: Science Press, 2000: 120(褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京:科学出版社,2000:120) [17] Lin L C. Acta Metall, 1987; 35: 1663 [18] Floris K M, Dauskardt R H. Acta Mater, 2001; 49, 2547 [19] Huang Y J. Amorphous Magnetic Physics and Materials.Xi'an: University of Electronic Science and TechnologyPress, 1991: 85(黄永杰.非晶态磁性物理与材料.西安:电子科技大学出版社1991:85) [20] Rooke D P, Cartwright D. J Compendium of Stress Intensity Factors. London: Her Majesty's Stationary Office, 1976: 274Q |
|