| 相场模型参数对枝晶形貌的影响 |
| 赵代平; 荆涛; 柳百成 |
| 清华大学机械工程系; 北京 100084 |
|
引用本文:
赵代平; 荆涛; 柳百成 . 相场模型参数对枝晶形貌的影响[J]. 金属学报, 2003, 39(8): 813-816 .
[1] Machiko O, Seong Gyoon K, Won Tae K, Toshio S. RecentISIJ int, 2001; 41: 1076 [2] Kobayashi R. Physica D, 1993; 63: 410 [3] Warren J A, Boettinger. Ada Mater, 1995; 43: 689 [4] Tiaden J, Nestler B, Diepers H J, Steinbach I. Physica D,1998; 115: 73 [5] Beckermann C, Diepers H J, Steinbach I, Karma A, TongX. J Comput Phys, 1999; 154: 468 [6] Nestler B, Wheeler A A, Ratke L, Stocker. Physica D,2000; 141: 133 [7] Karma A, Rappel W-J. Phys Rev E, 1999; 60: 3614 [8] Li Q, Beckermann C. Acta Mater, 1999; 47: 2345 [9] Karma A, Rappel W-J. Phys Rev E, 1998; 57: 4323 [10] Ihle T, Muller-Krumbhaar H. Phys Rev E, 1994; 49: 2972x |
|