| 坩埚旋转波形参数对晶体组分偏析影响的数值研究 |
| 刘俊成 |
| 山东理工大学材料科学与工程学院; 淄博 255091 |
|
| Simulation of Effect of Crucible Rotation Parameter on Single Crystal Solute Segregation |
| LIU Juncheng |
| School of Materials Science and Engineering; Shandong University of Technology; Zibo 255091 |
引用本文:
刘俊成 . 坩埚旋转波形参数对晶体组分偏析影响的数值研究[J]. 金属学报, 2004, 40(9): 987-994 .
.
Simulation of Effect of Crucible Rotation Parameter on Single Crystal Solute Segregation[J]. Acta Metall Sin, 2004, 40(9): 987-994 .
[1] Schulz-Dubois E O. J Cryst Growth, 1971; 12: 81 [2] Capper P, Gosney J J G, Jones C L, Pearce E J. J ElectronMater, 1986; 15: 361 [3] Distanov V E, Kirdyashkin A G. J Cryst Growth, 2001;222: 607 [4] Capper P, Gosney J J G, Jones C L, Kenworthy I. J Electron Mater, 1986; 15: 371 [5] Capper P. Prog Cryst Growth Charact, 1989; 19: 259 [6] Capper P, Harris J E, Okeeffe E S. Adv Mater Opt Electron, 1995; 5: 101 [7] Capper P. J Mater Sci-Mater Electron, 2001; 12: 423 [8] Brice J C, Capper P, Jones C L, Gosney J J G. Prog CrystGrowth Charact, 1986; 13: 197 [9] Liu J C, Jie W Q, Zhou Y H. Ada Metall Sin, 1996; 32: 269(刘俊成,介万奇,周尧和.金属学报, 1996;32:269) [10] Liu J C, Jie W Q, Zhou Y H. Prog Nat Sci, 1997; 7: 215 [11] Liu J C, Jie W Q. J Cryst Growth, 1998; 183: 140 [12] Yeckel A, Derby J J. J Cryst Growth, 2000; 210: 734 [13] Sen S, Konkel W H.Tighe S J, Bland L G, Sharma S R,Taylor R E. J Cryst Growth, 1988; 86: 111 [14] Rudolph P, Muhlberg M. Mater Sci Eng, 1993; B16: 8 [15] Aslam N, Jones E, Noakes T C Q, Mullin J B, WilloughbyF W. J Cryst Growth, 1992; 117: 249 [16] Liu J C. Prog Nat Sci, 2003; 13: 1293(刘俊成.自然科学进展,2003;13:1293) [17] Liu X H, Jie W Q, Zhou Y H. J Cryst Growth, 2000; 209:751 [18] Liu X H, Jie W Q, Zhou Y H. J Cryst Growth, 2000; 219:22 [19] Yeckel A, Derby J J. J Cryst Growth, 2001; 233: 599 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|