| 反应球磨中Mg的直接氢化 |
| 王平 张海峰 |
| 中国科学院金属研究所快速凝固非平衡合金国家重点实验室验室; 沈阳 110015 |
|
引用本文:
王平; 张海峰 . 反应球磨中Mg的直接氢化[J]. 金属学报, 2000, 36(10): 1118-1120 .
[1] Song M Y, Ivanov E, Darriet B, Pezat M, Hagenmuller P.J Less-Common Met, 1987; 131: 71 [2] Terzieva M, Khrussanova M, Peshev P. i Alloys Compd,1998; 267: 235 [3] Liang G, Boily S, Huot J, Van Neste A, Schulz R. J AlloysCompd, 1998; 268: 302. [4] Gross K J, Spatz P, Zuttel, Schlapbach L. J Alloys Compd,1997; 267: 276 [5] Dutta K, Srivastava O N. J Mater Sci, 1993; 28: 3457 [6] Gross K J, Spatz P, Zuttel A, Schlapbach L. J AlloysCompd, 1996; 240: 206 [7] Schulz R, Huot J, Liang G, Boily S, Lalande G, Dents MC, Dodelet J P. Mater Sci Eng, 1999; A267: 240 [8] Orimo S, Fujii H, Ikeda K. Acta Mater 1997; 45: 331 [9] Orimo S, Ikeda K, Fujii H, Fujikawa Y, Kitano K, Yamamoto K. Acta Mater, 1997; 45: 2271 [10] Small D A, Mackay G R, Dunlap R A. J Alloys Compd,1999; 284: 312 [11] Bortz M, Bertheville B, Buttger G, Yvon K. J AlloysCompd, 1999; 287: L4 [12] Wang P, Wang A M, Wang Y L, Zhang H F, Hu Z Q. ScrMater, accepted [13] Zaluski L, Zaluska A, Strom-Olsen J O. J Alloys Compd,1997; 253: 70 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|