| 高温热处理对(DS)NiAl--Cr(Mo)--Hf共晶合金显微组织和显微硬度的影响 |
| 徐春梅;郭建亭 |
| 中国科学院金属研究所 |
|
| Influence Of High Temperature Heat Treatment On Microstructure And Microhardness Of (Ds)Nial--Cr(Mo)—Hf Eutectic Alloy |
| XU Chunmei; GUO Jianting |
| Institute of Metal Research; The Chinese Academy of Sciences |
引用本文:
徐春梅; 郭建亭 . 高温热处理对(DS)NiAl--Cr(Mo)--Hf共晶合金显微组织和显微硬度的影响[J]. 金属学报, 2004, 40(1): 57-61 .
,
.
Influence Of High Temperature Heat Treatment On Microstructure And Microhardness Of (Ds)Nial--Cr(Mo)—Hf Eutectic Alloy[J]. Acta Metall Sin, 2004, 40(1): 57-61 .
[1] Walter J L, Cline H E. Metall Trans, 1970; 1:1221 [2] Cline H E, Waiter J L. Metall Trans, 1970; 1:2907 [3] Heredia F E, He M Y, Lucas G E, Evans A G, Deve H E, Konitzer D. Acta Metall Mater, 1993; 41:505 [4] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whit tenberger J D. Intermetalics, 1995; 3:99 [5] Polvani R S, Tzeng W S, Strutt P R. Metall Trans, 1976; 7A: 33 [6] Bowman R R, Noebe R D, Raj S V, Locci I E. Metall Trans, 1992; 23A: 1493 [7] Chen R S, Guo J T, Zhou J Y. Mater Lett, 2000; 42:80 [8] Cui C Y, GUO J T. Acta Metall Sin, 1999; 35:477(崔传勇,郭建亭.金属学报,1999;35:477) [9] Qi Y H, Guo J T, Cui C Y, Li G S. Mater Eng, 2001; 7: 15(齐义辉,郭建亭,崔传勇,李谷松.材料工程,2001;7:15) [10] Yang J M, Jeng S M, Bain K, Amato R A. Acta Mater, 1997; 45:295 [11] Cui C Y, Guo J T, Qi Y H, Ye H Q. Intermetallics, 2002; 10:1001 [12] Cui C Y, Chen Y X, Guo J T, Qi Y H, Ye H Q. Mater Sci Eng, 2002; A325:186 [13] Chen X F, Johnson D R, Noebe R D, Oliver B F. J Mater Res, 1995; 10:1159 [14] Jiang D T, Guo J T. Mater Lett, 1998; 36:33 |
|