| 间隙元素O对 β 型Ti-15Mo合金超低温力学性能的影响 |
戴进财1, 闵小华1( ), 辛社伟2, 刘凤金1 |
1 大连理工大学 材料科学与工程学院 大连 116024 2 西北有色金属研究院 西安 710016 |
|
| Effect of Interstitial Element O on Cryogenic Mechanical Properties in β-Type Ti-15Mo Alloy |
DAI Jincai1, MIN Xiaohua1( ), XIN Shewei2, LIU Fengjin1 |
1 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China 2 Northwest Institute for Non-Ferrous Metal Research, Xi'an 710016, China |
引用本文:
戴进财, 闵小华, 辛社伟, 刘凤金. 间隙元素O对 β 型Ti-15Mo合金超低温力学性能的影响[J]. 金属学报, 2025, 61(2): 243-252.
Jincai DAI,
Xiaohua MIN,
Shewei XIN,
Fengjin LIU.
Effect of Interstitial Element O on Cryogenic Mechanical Properties in β-Type Ti-15Mo Alloy[J]. Acta Metall Sin, 2025, 61(2): 243-252.
| 1 |
Xu A J, Wan H F, Liang C Z, et al. Application status and development trend of cryogenic titanium alloy [J]. J. Netshape Form. Eng., 2020, 12(6): 145
|
| 1 |
许爱军, 万海峰, 梁春祖 等. 低温钛合金材料应用现状及发展趋势 [J]. 精密成形工程, 2020, 12(6): 145
|
| 2 |
Huang C W, Ge P, Zhao Y Q, et al. Research progress in titanium alloys at cryogenic temperatures [J]. Rare Met. Mater. Eng., 2016, 45: 254
|
| 2 |
黄朝文, 葛 鹏, 赵永庆 等. 低温钛合金的研究进展 [J]. 稀有金属材料与工程, 2016, 45: 254
|
| 3 |
Osamu U. Review of the mechanical properties of high-strength alloys at cryogenic temperatures [J]. Mater. Perform. Charact., 2021, 10: 3
|
| 4 |
Yu Y, Jiang P, Li S K. Recent advances in the development and application of cryogenic titanium alloys [J]. Dev. Appl. Mater., 2014, 29(6): 118
|
| 4 |
郁 炎, 蒋 鹏, 李士凯. 国内外低温钛合金的开发与应用现状 [J]. 材料开发与应用, 2014, 29(6): 118
|
| 5 |
Leyens C, Peters M. Titanium and titanium alloys [M]. Weinheim: Wiley-VCH Verlag GmbH & Co. KGaA, 2003: 36
|
| 6 |
Lei L, Zhao Q Y, Zhu Q W, et al. Twinning-induced high impact toughness of titanium alloy at cryogenic temperature [J]. Mater. Sci. Eng., 2022, A860: 144258
|
| 7 |
Lu Z C, Zhang X H, Ji W, et al. Investigation on the deformation mechanism of Ti-5Al-2.5Sn ELI titanium alloy at cryogenic and room temperatures [J]. Mater. Sci. Eng., 2021, A818: 141380
|
| 8 |
Nayan N, Singh G, Prabhu T A, et al. Cryogenic mechanical properties of warm multi-pass caliber-rolled fine-grained titanium alloys: Ti-6Al-4V (normal and ELI grades) and VT14 [J]. Metall. Mater. Trans., 2018, 49A: 128
|
| 9 |
Singh G, Bajargan G, Datta R, et al. Deformation and strength of Ti-6Al-4V alloyed with B at cryogenic temperatures [J]. Mater. Sci. Eng., 2014, A611: 45
|
| 10 |
Lu Z C, Sun Y C, Yao C G, et al. Microstructure and mechanical properties of novel Ti-Al-V-Zr-Mo-Nb cryogenic titanium alloy [J]. Rare Met. Mater. Eng., 2022, 51: 217
|
| 10 |
陆子川, 孙亚超, 姚草根 等. 一种新型Ti-Al-V-Zr-Mo-Nb低温钛合金组织与性能研究 [J]. 稀有金属材料与工程, 2022, 51: 217
|
| 11 |
Zang M C, Niu H Z, Zhang H R, et al. Cryogenic tensile properties and deformation behavior of a superhigh strength metastable beta titanium alloy Ti-15Mo-2Al [J]. Mater. Sci. Eng., 2021, A817: 141344
|
| 12 |
Xiang L, Min X H, Mi G B. Application and research progress of body-centered-cubic Ti-Mo base alloys [J]. J. Mater. Eng., 2017, 45(7): 128
doi: 10.11868/j.issn.1001-4381.2016.000737
|
| 12 |
向 力, 闵小华, 弭光宝. 体心立方Ti-Mo基钛合金应用研究进展 [J]. 材料工程, 2017, 45(7): 128
|
| 13 |
Zhang S J, Min X H, Li Y D, et al. Effects of deformation and phase transformation microstructures on springback behavior and biocompatibility in β-Type Ti-15Mo alloy [J]. Acta Metall. Sin. (Engl. Lett.), 2022, 35: 621
|
| 14 |
Dai J C, Min X H, Zhou K S, et al. Coupling effect of pre-strain combined with isothermal ageing on mechanical properties in a multilayered Ti-10Mo-1Fe/3Fe alloy [J]. Acta Metall. Sin., 2021, 57: 767
|
| 14 |
戴进财, 闵小华, 周克松 等. 预变形与等温时效耦合作用下Ti-10Mo-1Fe/3Fe层状合金的力学性能 [J]. 金属学报, 2021, 57: 767
doi: 10.11900/0412.1961.2020.00286
|
| 15 |
Yao K, Xin S W, Yang Y, et al. Ultrahigh cryogenic strength and exceptional ductility at 20 K in a TWIP Ti-15Mo alloy [J]. Scr. Mater., 2022, 213: 114595
|
| 16 |
Chong Y, Poschmann M, Zhang R P, et al. Mechanistic basis of oxygen sensitivity in titanium [J]. Sci. Adv., 2020, 6: 4060
|
| 17 |
Wasz M L, Brotzen F R, Mclellan R B, et al. Effect of oxygen and hydrogen on mechanical properties of commercial purity titanium [J]. Int. Mater. Rev., 1996, 41: 1
|
| 18 |
Min X H, Emura S, Tsuchiya K, et al. Transition of multi-deformation modes in Ti-10Mo alloy with oxygen addition [J]. Mater. Sci. Eng., 2014, A590: 88
|
| 19 |
Min X H, Bai P F, Emura S, et al. Effect of oxygen content on deformation mode and corrosion behavior in β-type Ti-Mo alloy [J]. Mater. Sci. Eng., 2017, A684: 534
|
| 20 |
Kim J I, Kim H Y, Hosoda H, et al. Shape memory behavior of Ti-22Nb-(0.5-2.0)O (at%) biomedical alloys [J]. Mater. Trans., 2005, 46: 852
|
| 21 |
Min X H, Xiang L, Li M J, et al. Effect of {332}<113> twins combined with isothermal ω-phase on mechanical properties in Ti-15Mo alloy with different oxygen contents [J]. Acta Metall. Sin., 2018, 54: 1262
|
| 21 |
闵小华, 向 力, 李明佳 等. {332}<113>孪晶与等温ω相的组合对不同O含量Ti-15Mo合金力学性能的影响 [J]. 金属学报, 2018, 54: 1262
doi: 10.11900/0412.1961.2018.00022
|
| 22 |
Yao K, Min X H. Abnormal strain rate strengthening and strain hardening with constitutive modeling in body-centered cubic {332}<113> TWIP titanium alloy [J]. Acta Mater., 2022, 226: 117641
|
| 23 |
Li M J, Min X H, Yao K, et al. Novel insight into the formation of α″-martensite and ω-phase with cluster structure in metastable Ti-Mo alloys [J]. Acta Mater., 2019, 164: 322
|
| 24 |
Wang K G, Deng Z X, Tian Y Y, et al. Effect of cold rolling and solution treatment on β stability and mechanical properties of a metastable β-Ti alloy [J]. Mater. Sci. Eng., 2022, A861: 144366
|
| 25 |
Yao K, Min X H, Emura S, et al. Coupling effect of deformation mode and temperature on tensile properties in TWIP type Ti-Mo alloy [J]. Mater. Sci. Eng., 2019, A766: 138363
|
| 26 |
Qu L, Yang Y, Lu Y F, et al. A detwinning process of {332}<113> twins in beta titanium alloys [J]. Scr. Mater., 2013, 69: 389
|
| 27 |
Gutierrez-Urrutia I, Li C L, Emura S, et al. Study of {332}<113> twinning in a multilayered Ti-10Mo-xFe (x = 1-3) alloy by ECCI and EBSD [J]. Sci. Technol. Adv. Mater., 2016, 17: 220
|
| 28 |
Boyer R, Collings E W, Welsch G. Materials Properties Handbook: Titanium Alloys [M]. Materials Park: ASM International, 1994: 68
|
| 29 |
Zang M C, Niu H Z, Liu S, et al. Achieving highly promising strength-ductility synergy of powder bed fusion additively manufactured titanium alloy components at ultra-low temperatures [J]. Addit. Manuf., 2023, 65: 103444
|
| 30 |
Antony Prabhu T, Murugesan N, Thomas Tharian K, et al. Studies on mechanical properties of Ti-6Al-4V ELI at liquid hydrogen temperature [J]. Mater. Sci. Forum, 2015, 830-831: 207
|
| 31 |
Di iorio S, Briottet L, Rauch E F, et al. Plastic deformation, damage and rupture of PM Ti-6Al-4V at 20 K under monotonic loading [J]. Acta Mater., 2007, 55: 105
|
| 32 |
Hanada S, Izumi O. Transmission electron microscopic observations of mechanical twinning in metastable beta titanium alloys [J]. Metall. Trans., 1986, 17A: 1409
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|