| Mn和In添加对SmCo7结构稳定性及磁矩影响的第一性原理计算 |
毛斐, 吕皓, 唐法威, 郭凯, 刘东, 宋晓艳( ) |
| 北京工业大学 材料与制造学部 新型功能材料教育部重点实验室 北京 100124 |
|
| First-Principle Calculation on the Effect of Mn and In on the Structural Stability and Magnetic Moment of SmCo7 Alloys |
MAO Fei, LU Hao, TANG Fawei, GUO Kai, LIU Dong, SONG Xiaoyan( ) |
| Key Laboratory of Advanced Functional Materials, Ministry of Education, Facaulty of Materials and Manufacturing, Beijing University of Technology, Beijing 100124, China |
引用本文:
毛斐, 吕皓, 唐法威, 郭凯, 刘东, 宋晓艳. Mn和In添加对SmCo7结构稳定性及磁矩影响的第一性原理计算[J]. 金属学报, 2021, 57(7): 948-958.
Fei MAO,
Hao LU,
Fawei TANG,
Kai GUO,
Dong LIU,
Xiaoyan SONG.
First-Principle Calculation on the Effect of Mn and In on the Structural Stability and Magnetic Moment of SmCo7 Alloys[J]. Acta Metall Sin, 2021, 57(7): 948-958.
| 1 |
Gutfleisch O, Willard M A, Brück E, et al. Magnetic materials and devices for the 21st century: Stronger, lighter, and more energy efficient [J]. Adv. Mater., 2011, 23: 821
|
| 2 |
Liu J F, Chui T, Dimitrov D, et al. Abnormal temperature dependence of intrinsic coercivity in Sm(Co, Fe, Cu, Zr)z powder materials [J]. Appl. Phys. Lett., 1998, 73: 3007
|
| 3 |
Seyring M, Song X Y, Zhang Z X, et al. Concurrent ordering and phase transformation in SmCo7 nanograins [J]. Nanoscale, 2015, 7: 12126
|
| 4 |
Buschow K H J. New developments in hard magnetic materials [J]. Rep. Progr. Phys., 1991, 54: 1123
|
| 5 |
Zhang Z X, Song X Y, Li D P, et al. Phase stability and phase transformation of nanocrystalline SmCo7 alloy and their effects on the magnetic performance [J]. Rare. Met. Mater. Eng., 2013, 42: 565
|
| 5 |
张哲旭, 宋晓艳, 李定朋等. 纳米晶SmCo7合金的相稳定性、相变行为及其对磁性能的影响 [J]. 稀有金属材料与工程, 2013, 42: 565
|
| 6 |
Hirosawa S, Nishino M, Miyashita S. Perspectives for high-performance permanent magnets: Applications, coercivity, and new materials [J]. Adv. Nat. Sci: Nanosci. Nanotechnol., 2017, 8: 013002
|
| 7 |
Sun J B, Bu S J, Ding H W, et al. The effects of CNTs and/or Si additions on the structure and magnetic properties of SmCo7-based alloys [J]. J. Alloys Compd., 2013, 563: 91
|
| 8 |
Al-Omari A I, Yeshurun Y, Zhou J, et al. Magnetic and structural properties of SmCo7-xCuxalloys [J]. J. Appl. Phys., 2000, 87: 6710
|
| 9 |
Zhou J, Al-Omari A I, Liu J P, et al. Structure and magnetic properties of SmCo7-xTixwith TbCu7-type structure [J]. J. Appl. Phys., 2000, 87: 5299
|
| 10 |
Hsieh C C, Huang S T, Guo J S, et al. Effect of a carbon additive on the TbCu7-type melt-spun Sm(Co, M)7 (M = Ti, Zr, Hf, V and Ge) ribbons [J]. J. Korean Phys. Soc., 2013, 63: 401
|
| 11 |
Zaigham H, Khalid F A. Exchange coupling and magnetic behavior of SmCo5-xSnx alloys [J]. J. Mater. Sci. Technol., 2011, 27: 218
|
| 12 |
Hsieh C C, Chang H W, Guo Z H, et al. Crystal structure and magnetic properties of melt spun SmCo7-xMx (M = Ta, Cr, and Mo; x = 0-0.6) ribbons [J]. J. Appl. Phys., 2010, 107: 09A738
|
| 13 |
Hsieh C C, Shih C W, Liu Z, et al. Magnetic properties and crystal structure of melt spun Sm(Co, M)7 (M = Al and Si) ribbons [J]. J. Appl. Phys., 2012, 111: 07E306
|
| 14 |
Hua G, Song X Y, Liu D, et al. Effects of Hf on phase structure and magnetic performance of nanocrystalline SmCo7-type alloy [J]. J. Mater. Sci., 2016, 51: 3390
|
| 15 |
Qian J W, Guo Y Q. Effect on the structure stability of minor Al or Zn doping into SmCo7 [A]. DEStech Transactions on Materials Science and Engineering [C]. Sanya: DEStech Publications, 2017: 83
|
| 16 |
Luo J, Liang J K, Guo Y Q, et al. Effects of the doping element on crystal structure and magnetic properties of Sm(Co, M)7, compounds (M = Si, Cu, Ti, Zr, and Hf) [J]. Intermetallics, 2005, 13: 710
|
| 17 |
Chen Y Y, Hsieh C C, Lo S C, et al. The effect of doping element Zr on anisotropy and microstructure of SmCo7-xZrx [J]. J. Appl. Phys., 2011, 109: 07A748
|
| 18 |
Sun J B, Bu S J, Yang W, et al. Structure and magnetic properties of SmCo7-xGax (0 ⩽ x ⩽ 1.2) alloys [J]. J. Alloys Compd., 2014, 583: 554
|
| 19 |
Li Y Y, Jiang S, Chen Y. Atomistic simulation for disordered TbCu7-type compounds SmCo7 and Sm(Co,T)7 (T = Ti, Ga, Si, Cu, Hf, Zr) [J]. Solid State Sci., 2010, 12: 33
|
| 20 |
Liu D, Guo K, Tang F W, et al. Selecting doping elements by data mining for advanced magnets [J]. Chem. Mater., 2019, 31: 10117
|
| 21 |
Mao F. First-principles calculations on structure and magnetism properties of Sm-Co based alloys [D]. Beijing: Beijing University of Technology, 2020
|
| 21 |
毛 斐. Sm-Co合金体系相结构与磁学性能的第一性原理计算研究 [D]. 北京: 北京工业大学, 2020
|
| 22 |
Zhang C W. Study on the electronic structure and magnetic properties of a new Sm-Co-based ternary permanent magnet alloy [D]. Jinan: Shandong University, 2006
|
| 22 |
张昌文. 新型Sm-Co基三元永磁合金的电子结构及磁性研究 [D]. 济南: 山东大学, 2006
|
| 23 |
Zhang Z X. Preparation and characterizations on structures and properties of nanocrystalline metastable samarium-cobalt alloys [D]. Beijing: Beijing University of Technology, 2012
|
| 23 |
张哲旭. 纳米晶Sm-Co亚稳相合金的制备及结构性能研究 [D]. 北京: 北京工业大学, 2012
|
| 24 |
Hua G. Effects of metallic element doping on phase stability and magnetic performance of metastable SmCo7-type alloys [D]. Beijing: Beijing University of Technology, 2016
|
| 24 |
华 刚. 添加金属元素对SmCo7亚稳相合金稳定性和磁性能的影响 [D]. 北京: 北京工业大学, 2016
|
| 25 |
Kresse G, Furthmüller J. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set [J]. Phys. Rev., 1996, 54B: 11169
|
| 26 |
Kresse G, Furthmüller J. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set [J]. Comput. Mater. Sci., 1996, 6: 15
|
| 27 |
Perdew J P, Chevary J A, Vosko S H, et al. Atoms, molecules, solids, and surfaces: Applications of the generalized gradient approximation for exchange and correlation [J]. Phys. Rev., 1992, 46B: 6671
|
| 28 |
Perdew J P, Burke K, Ernzerhof M. Generalized gradient approximation made simple [J]. Phys. Rev. Lett., 1996, 77: 3865
|
| 29 |
Andreev A V, Zadvorkin S M. Thermal expansion and spontaneous magnetostriction of RCo5 intermetallic compounds [J]. Physica, 1991, 172B: 517
|
| 30 |
Kohan A F, Ceder G, Morga D, et al. First-principles study of native point defects in ZnO [J]. Phys. Rev., 2000, 61B: 15019
|
| 31 |
Condon E U. The principles of statistical mechanics [J]. J. Appl. Phys., 1939, 10: 691
|
| 32 |
Dixit V, Nandadasa C N, Kim S G, et al. Site occupancy and magnetic properties of Al-substituted M-type strontium hexaferrite [J]. J. Appl. Phys., 2015, 117: 243904
|
| 33 |
van de Walle A, Ceder G. The effect of lattice vibrations on substitutional alloy thermodynamics [J]. Rev. Mod. Phys., 2002, 74: 11
|
| 34 |
Xu Z Y. Thermodynamics of Materials [M]. Beijing: Higher Education Press, 2009: 52
|
| 34 |
徐祖耀. 材料热力学 [M]. 北京: 高等教育出版社, 2009: 52
|
| 35 |
Hua G, Song X Y, Tang F W, et al. Modeling and experimental studies of Hf-doped nanocrystalline SmCo7 alloys [J]. CrystEngComm., 2016, 18: 8080
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|