| 含Ti高炉渣冷却及析晶过程中导率的变化 |
| 王淑兰 李光强 隋智通 |
| 东北大学材料与冶金学院;沈阳 110006 |
|
引用本文:
王淑兰; 李光强; 隋智通 . 含Ti高炉渣冷却及析晶过程中导率的变化[J]. 金属学报, 1999, 35(5): 499-502 .
[1]Du H G. Smelting Principle of Vanadium-Bearing Titano-magnetite by Blast Furnace. Beijing: Science Press, 1997:20(杜鹤桂.高炉治炼钒钛磁铁矿原理.北京:科学出版社,1997:20) [2] Lou T P, Li Y H, Ma J W, Xia Y H, Sui Z T. Acta MetallSin, 1999; 35(to be published)(娄太平,李玉海,马俊伟,夏玉虎,随智通,金属学报,1999;35(待发表) [3] Schiefelbein S L, Sadoway D R. Metall Mater aams, 1997;28B: 1141 [4] Allibert M. Verein Deutscher Eisenhuttenleute (VDEH). Slagatlas. 2nd ed, Gmbh: Verlag Stahleisen Press, 1995: 559 [5] Jiao Q, Themelis N J. Metall aams, 1988; 19B: 133 [6] Hu Y, Lh R D, Liu G J, Lu Y N. Physical Chemistry. 3rded, Beijing: High Education Press, 1998: 223(胡英,吕瑞东,刘国杰.陆曜南.物理化学下册(第三版). 北京:高等教育出版社,1988: 223)2 |
|