| Al, Ti和Nb对Fe-Ni-Cr-Co-Nb-Ti-Al合金铸态组织的影响 |
| 刘雅晶 李玉清 谢锡善 J.H.Tundermann 董建新 郭晓倬 |
| 大冶特殊钢股份有限公司技术中心;黄石 435001 |
|
引用本文:
刘雅晶; 李玉清; 谢锡善; J.H.Tundermann; 董建新; 郭晓倬 . Al, Ti和Nb对Fe-Ni-Cr-Co-Nb-Ti-Al合金铸态组织的影响[J]. 金属学报, 1999, 35(10): 1036-1042 .
[1] Jackman L A, Maurer G E, Widge S. In: Swaminathan V P, Cheruvu N S eds., Advanced Materials and Coatings for Combustion Turbines, Metals Park, Ohio: ASM Interna-tional, Member/Custormer Center, 1994: 43 [2] Chang K M, Lai H J, Hwang J Y. In: Loria E A ed., Su-peralloys 718,625,7o6 and Various Derivatives, Warrendale:The Minerals, Metals & Materials Society, 1994: 683 [3] Okaxaki Y, Ichikawa K, Matsuo M. J Jpn Inst Met, 1991;55: 729(畸义光,市川洌,松尾宗次。日本金属学会志, 1991; 55: 729) [4] Baldan A. In: Bachelet E, Brunetaud R, Coutsouradis Deds., High Temperature Materials for Power Eapineering 1990, Vol.II, The Netherland: Kluwer Academic Publishers,1990: 1329 [5] Tianyi C, Shouhya Z. J Mater Sci Lett, 1990; 9: 820 [6] Zhang J, Zhang Z, Tang Y. In: Liu C T, Taub A I, Stoloff NS, Koch C C eds., High- Temperature 0ndered IntermetallicAllogs, Pittsburgh: Materials Research Society 1989: 549 [7] Li Y Q, Liu J Y. Interstitial Phases at Grain Boundariesin Superalloys. Beijing: Metallurgical Industry Press, 1990:269(李玉清, 刘锦岩. 高温合金晶界间隙相。北京: 冶金工业出版社,1990: 269) [8] Huang X Y. Transmission Electron Microscopy.Shanghai:Shanghai Science and Technology Press, 1987: 362(黄孝瑛。透射电子显微学. 上海:上海科学技术出版社,1987:362) [9] Li Y Q, Li P, Liu Y J. Prog Nat Sci, 1998; 8: 611(李玉汪,李蓬,刘晶,自然科学进展,1998; 8: 611) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|